Litlhokomelo Bakeng sa Ferritic Stainless Steel Continuous Casting
Ha e bapisoa le austenitic celik, ferritic celik e na le matla a holimo a lihlahisoa. Tlas'a maemo a ts'oanang a ts'ebetso, lisebelisoa tse nang le likarolo tse nyane li ka sebelisoa ho boloka litšenyehelo; Ntle le moo, tšepe e sa hloekang ea ferritic ha e na Ni (tse khethehileng li na le palo e nyane feela), litšenyehelo li tlase haholo. Ka hona, tlhahiso le ts'ebeliso ea tšepe e sa hloekang ea ferritic e khahlile batho.
Ts'ebetso e tsoelang pele ea ho lahla tšepe e sa hloekang ea ferritic e batla e khethehile. Taolo e sa utloahaleng e tloaetse ho ba le mathata a joalo ka mapatso a bokaholimo, ho phatloha, mapetso a kahare a bakoang ke ho phatloha, khethollo ea bohareng, le sekhahla se tlase sa kristale se lekanang. Ela hloko lintlha tse kaholimo tlhahiso:
1. Mokotla o moholo
Hobane ho na le lintho tse ling tse qhibilihisang haholo (Cr2O3, Al2O3, jj.) Ka tšepe e sa hloekang e entsoeng ka tšepe e qhibilihisitsoeng, viscosity ea tšepe e qhibilihisitsoeng e phahame, e fokotsang ho qhibiliha ha tšepe e qhibilihisitsoeng, mme nozzle e sekametse ho maqhutsu le e hatsela ho isa lefung.
Ka hona, e lokela ho ba le mosebetsi o ikemetseng oa ho paka likhahla ho fokotsa lerotholi la mocheso oa tšepe e qhibilihisitsoeng nakong ea ts'ebetso, mme ka nako e ts'oanang ho foka oksijene ho hlokahala ho netefatsa tsoelo-pele ea ho betsa.
2. Tundish
Ho na le lintho tse ngata tse qhibilihisang haholo ka tšepe e sa hloekang, 'me viscosity ea tšepe e qhibilihisitsoeng e phahame. Kamora hore tšepe e qhibilihisitsoeng e kenngoe ka har'a seretse, ho bonolo ho theha moferefere le ho ts'oaroa ha slag.
Moralong oa tundish, ho lokela ho sebelisoa letamo le qhibilihisitsoeng le nang le matla a maholo mme sesebelisoa sa taolo ea phallo (lebota la slag, letamo la slag, jj.) Se lokela ho eketsoa ho lelefatsa nako ea bolulo ea tšepe e qhibilihisitsoeng ho tundish le netefatsa hore inclusions ka tšepe e qhibilihisitsoeng ke hlobo phofo absorption le assimilation. Ntle le moo, ha o fetola sephutheloana se seholo, mokelikeli oa tšepe e tundish e ke ke ea theoloa haholo ho thibela vortex le slag.
3. Moetsi oa 'mala
Hlobo e tsoang ho ferritic celik foromeletsoeng billet e angoa habonolo ke khatello ea hydrostatic ea tšepe e qhibilihisitsoeng, 'me bophara le botenya ba eona ba ba kholoanyane kapa baka likoli bulging. Ka hona, sesebelisoa sa phetoho ea bophara ba hlobo se tlameha ho sebelisa phetoho ea servo-hydraulic hole e ka fetolang ho bula le ho tepa habonolo. Motsoako o moholo oa phetoho ea kristale o na le phetoho e futhumatsang mohala le ho notlela ka boeona ho netefatsa hore taper e tsitsitse ho ± 0.2 mm, e le ho ikamahanya le phetoho ea taper le ho bula maemong a fapaneng a ho tšela.
4. Phallo ea taolo ea boemo ba metsi
Boemo ba mokelikeli oa hlobo bo sebelisa silindara sa motlakase ho laola mokhoa oa ho bula le ho koala oa molamu oa tundish ho thibela phallo e sa lekanang ea hlobo ea hlobo le ho qoba litšitiso tse kaholimo ho marang-rang le likhoele tsa slag.
5. Theknoloji ea Hydraulic vibration
Ts'epe e sa hloekang ea Ferritic e na le matla a tlase a mocheso o phahameng le viscosity e phahameng ea tšepe e qhibilihisitsoeng. Mofuta oa "amplitude low", "frequency frequency" ea ho sisinyeha e ka rarolla liphoso tse kang mapatso a marang-rang le matšoao a tebileng a thothomelo.
6. Serame sa bobeli
Ts'epe e sa hloekang ea Ferritic ha e utloisise mocheso o phahameng oa mocheso, kahoo metsi a tšepe e sa hloekang a phahame ho feta a martensitic le austenitic stainless steel, ke hore, metsi a itseng a ferrite> metsi a itseng austenite> metsi a itseng bophahamo ba modumo ea martensite.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape:Litlhokomelo Bakeng sa Ferritic Stainless Steel Continuous Casting
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off