The Mabaka a Aluminium shoa lahla banana leaf Easy Cracking
Joalokaha bohle re tseba, aluminium alloy die die-casting die e tla ba le mapetso kamora nako ea tlhahiso.
Mabaka a mantlha a ketsahalo ena ke a latelang:
- Mocheso oa hlobo o phahame haholo 'me khatello ea kelello e kholo haholo
- Hlobo hlobo thepa ea mantlha e sebelisa 8407, skd61
- The hlobo mocheso kalafo thatafala e phahameng haholo
- Tlhokomelo ea kamehla, makhetlo a 5k makhetlo a 1, makhetlo a 15k1 tempering makhetlo a 30k ……
Ho thibela lefu lahla hlobo le ho eketsa bophelo ba ts'ebeletso ea tšepe ea hlobo e tsoang kantle
Lintlha tse latelang li tlameha ho etsoa:
- 1. Litlhokahalo tsa kalafo ea mocheso ea karolo e etsang karolo ea hlobo e lahlang (e tsamaeang, konokono ea hlobo, konokono): thatafalo e tlameha ho netefatsoa hore e tla ba HRC43 ~ 48 (thepa e ka ba SKD61 kapa 8407)
- 2. hlobo e lokela ho futhumatsoa ka botlalo pele e hlahisoa. Mesebetsi ea eona ke e latelang:
- 2.1 Etsa hlobo hore e fihle boemong bo botle ba mocheso, etsa sekhahla sa ho tiisa sekhahla le ho nolofalletsa phetisetso ea khatello.
- 2.2 Boloka mokelikeli oa motsoako o shoang ha o tlatsitsoe, o na le boits'oaro bo botle mme o ntlafatsa boleng ba bokaholimo.
- 2.3 Fokotsa liphoso tsa tlhahiso ea pele ho nako le ho ntlafatsa tlhahiso ea batho ba shoang.
- 2.4 Fokotsa khatello ea kelello e futhumatsang ea hlobo ebe o eketsa bophelo ba ts'ebeletso ea hlobo. Litlhaloso tse ikhethang ke tse latelang:
Kamora hore hlobo e ncha e hlahisoe nako e telele
Ho bokellana ha khatello ea mocheso ke sesosa se tobileng sa ho petsoha ha hlobo ea hlobo. Bakeng sa ho fokotsa khatello ea kelello ea mocheso, sebopeho sa hlobo le sekhahla se lokela ho halefisoa ho felisa khatello ea maikutlo kamora ho hlahisoa ka nako e itseng. itseng
Mekhoa ea tlhahiso e hlokang ho felisa khatello ea maikutlo ke e latelang:
Mofuta oa hlobo | Pele Tempering | Tempering ea bobeli | Tempering ea Boraro |
motsoako aluminium | <2000 makhetlo a hlobo | <10000 makhetlo a hlobo | <30000 makhetlo a hlobo |
Qiqea zloy | <10000 makhetlo a hlobo | <20000 makhetlo a hlobo | <50000 makhetlo a hlobo |
Malebela a 22 a ho etsa hore hlobo e fihle bophelong bo bolelele
- 1. Lisebelisoa tsa hlobo ea boleng bo holimo
- 2. Ka mokhoa o utloahalang meralo ea lebota la hlobo le litekanyo tse ling tsa hlobo
- 3. Leka ho sebelisa li-insert
- 4. Khetha sekhutlo se seholo ka ho fetisisa se ka khonehang tlasa maemo a teng
- 5. Sebaka se lipakeng tsa kanale ea metsi a pholileng le boemo le sekhutlo se tlameha ho ba kholo ka ho lekana
- 6. Bohale ba khatello ea maikutlo bo lokela ho tlosoa kamora mochini o thata
- 7. Kalafo ea mocheso e nepahetse, 'me ho tima le ho pholisa ho tlameha ho potlaka ka ho lekana
- 8. Senya ka botlalo 'me u tlose lera la scum la EDM
- 9. Boemo ha boa lokela ho bentšoa haholo
- 10. Bokaholimo ba hlobo bo lokela ho ba le oxidized
- 11. Haeba nitriding e khethang, lera la ho kenella ha lea lokela ho teba haholo
- 12. Preheat hlobo ho mocheso o khothalletsoang ka tsela e nepahetseng
- 13. Lebelo la hamore le liehang le lokela ho sebelisoa ho qala ho betsa likotoana tsa 5-10
- 14. Morero oa ho fumana lihlahisoa tse tšoanelehang, leka ho fokotsa mocheso oa aluminium e qhibilihisitsoeng ka hohle kamoo ho ka khonehang
- 15. Se ke oa sebelisa lebelo le phahameng haholo la mokelikeli oa aluminium
- Etsa bonnete ba hore hlobo e pholile hantle, 'me mocheso oa metsi a pholileng o lokela ho bolokoa ho 16 ~ 40 ℃
- 17. Bakeng sa ho koala nakoana, leka ho koala hlobo le ho fokotsa bongata ba metsi a pholileng ho qoba ho ts'oaroa ke mocheso ha o qala bocha
- 18. Setsidifatsi se lokela ho tingoa ha bokaholimo ba mohlala bo le mocheso o phahameng ka ho fetisisa
- 19. Ha se moemeli oa tokollo e ngata haholo
- 20. Kamora palo e itseng ea ho lahla, ho imolla khatello ea maikutlo le bohale
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape: The Mabaka a Aluminium shoa lahla banana leaf Easy Cracking
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off