1. Litšobotsi tsa Motheo tsa Aluminium Alloy
Japane ADCI2 aluminium-silicon alloy e na le ts'ebetso e ntle ea ho lahla, 'me ho lahla ho na le matla a holimo, coefficient e tlase ea ho holisa mocheso, ho hanyetsa ts'enyeho e phahameng le ts'ebetso e ntle ea chipping. Ka hona, e sebelisoa haholo ho hlahiseng koloi carburetor, cylinder block, cylinder head, le reducer ea literene.
Li-vibrator, li-gearbox tsa enjine, li-gearbox tsa mochini oa temo, 'mele ea likhamera,' mele ea lisebelisoa tsa motlakase le likarolo tse ling. Lilemong tsa morao tjena, ka kholo e potlakileng ea liindasteri tsa likoloi le tsa lithuthuthu, li sebelisitsoe haholo ho hlahisa matloana a pompo ea mariki bakeng sa likoloi tse nyane Le likhetla tsa motlakase tsa lithuthuthu le likarolo tse ling tse hlahisitsoeng ka bongata tse nyane le tse mahareng tse nang le libopeho tse rarahaneng. le matla a phahameng a nepahetseng.
Si | Fe | Cu | Mn | Mg | Ni | Zn | Sn | Pb |
9.6-12.0 | 1.8-3.5 |
Ka motsoako oa aluminium ADC12 castings, mohato oa al-Al ke sebopeho sa bohlokoahali. Boemong ba as-cast, mohato oa al-al o dendritic ebile o batla o le mahoashe, 'me moelelo oa ona ha o na tloaelo e itseng mme o mpa o le moferefere, o etsang hore ts'ebetso ea ona e se ntle haholo. ; Si ka motsoako e haholo-holo sebelisoa ho ntlafatsa ho betsa tshebetso, apara ho hanyetsa, ho hanyetsa ts'enyeho le thepa phetha molao feela. Cu le Mg ba theha mekhahlelo ea CuAl2 le Mg2Si ho matlafatsa alloy, empa haeba litaba li le holimo haholo, polasetiki e tla fokotseha, mme Cu e ka eketsa ts'ebetso ea mocheso o phahameng, empa e tla fokotsa ho hanyetsa ts'enyeho; Mn haholo-holo e theha karolo ea AIFeMnS, e fokotsa litlamorao tse mpe tsa litšila tsa Fe, mme e ka ntlafatsa ho hanyetsa mocheso oa castings. Fe ka kakaretso e nkuoa e le ntho e kotsi ka ho fetisisa ho litšila ho lits'epe tse kopantsoeng tsa Al. Karolo ea Fe ke karolo ea-Fe (AlgSiFez) le B-Fe (AIsSiFe). Karolo e thata le e bobebe ea acicular β-Fe e tla senya matla a khokahano ea matrix ea tšepe mme e fokotse haholo thepa ea mochini oa alloy (joalo ka matla a ho hanyetsa Tensile), Fe ho Al alloy e le ntho e kotsi e tla fokotsa haholo: thepa ea mochini ea alloy, e ama ho robeha hampe joalo-joalo.
2.The Process Of Aluminium Alloy Raw Materials Ho Laoloa
Matsatsing ana, boholo ba indasteri ea ho lahla thepa e reka li-ingots tsa motsoako oa aluminium ho tsoa ho lijalo tsa tlhahiso ea aluminium ingot. Li-ingots tsa aluminium tse lokisitsoeng tsa mofuta ona hangata li sebelisoa hape e le lihlahisoa tsa aluminium tsa bobeli e le sesebelisoa sa mantlha, mme sebopeho se fetotsoe (li-ingole tse hloekileng tsa aluminium le ba bang ba li-intermediates ba eketsoa). Motsoako). Ka hona, theko le theko ea thekiso ea motsoako ona oa aluminium ingot e tlase ho feta ea aluminium ingot e hloekileng e le sesebelisoa sa mantlha, empa litšila li phahame. Ka lebaka la boemo bona, ho hlokahala hore ho hlahlojoe lik'hemik'hale tsa li-ingots tsa aluminium tse rekiloeng, 'me u etse liphetoho tse nepahetseng ha u saena litlhoko tsa tekheniki le moetsi oa alloy aluminium ingot ho latela GB / T8733, ebe o hatela pele ho latela litlhoko ea die-cast aluminium alloy- Phetoho ea mehato. Ka lebaka la litlhoko tsa khase le lintlha tse thata ho motsoako oa aluminium, semela sa tlhahiso ea aluminium ingot se tlameha ho hloekisa, ho qhekella le ho hlaba litšila ho thibela likhase tse ngata le litšila tse ngata ho ingot ea aluminium hore e se futsetsoe mokelikeli oa aluminium. Ho hlokahala aluminium ingot Bokaholimo bo boreleli (kamora hore sekoli se tlosoe), ho robeha ho lokile 'me ha ho na lijo-thollo tse khanyang tsa kristale tsa silicone ea kristale. Mebubu ea moea e ka holim'a aluminium ingot ke hobane pente e hlobo ea ingot e na le metsi a mangata ebile ha e so omelloe. Bokaholimo ha bo phatsime hobane scum ha e so hlakoloe. Ho robeha ha ingot ea aluminium ho na le lithollo tse khanyang tsa kristale hobane mocheso o tšollang o phahame haholo mme ho na le likristale tsa silicon. Tlhahisong ea batho ba shoang, ho na le 30% ho 60% ea thepa e nchafalitsoeng. Haeba thepa e nchafalitsoeng e le mafura, e tlameha ho chesoa ebe e hatelloa ka mokelikeli oa aluminium. Sesepa sa aluminium se pshatlehileng se tlameha ho sefeoa le ho silafatsoa, 'me lehlabathe le lehlohlojane li tlameha ho tlosoa pele li khutlela seboping. Moo thepa e sebelisoang bocha e sebelisitsoeng Palo ea aluminium e qhibilihisitsoeng, moemeli oa ho hloekisa le ho tlosa slag e tlameha ho eketsoa ka nepo, 'me ka kakaretso e laoloe ho latela karolelano e kaholimo ea moeli. Ha o qhibilihisa, ingot ea aluminium e kenyellelitsoeng e tlameha ebe e omme.
3. Qhibiliha Of Aluminium motsoako
Sebōpi sa ho qhibilihisa se sebelisoang ke k'hamphani ke ATM-1500. Khamphani e hloka hore sebopi sa ho qhibilihisa se tlameha ho besoa nako le nako ha phetoho e buloa molemong oa ho tlosa mongobo seboping, mme sebopi kamora ho baka se tlameha ho fihlela litlhoko tse boletsoeng. Nakong ea ts'ebetso ea ho qhibilihisa, mocheso oa smelting oa hlokahala: (680 ~ 750) C; mocheso oa sebōpi o hloekisang: (730 + 10) C. Nakong ea ts'ebetso eohle ea ho qhibilihisa motsoako oa aluminium, tefiso e qala ho qhibiliha ha e futhumetse, e hlokomela phetoho ho tloha ho tiileng ho isa mokelikeli. Nakong ea ts'ebetso ena ea phetoho, tšepe e tla tšeloa mali, e chesoe ebe e fumana khase. Ho tšeloa ha tšepe le ho chesoa ha tšepe ho ke ke ha ama feela lik'hemik'hale tsa alloy, empa hape le kenyelletso ea slag e bakoang ke oxidation ke e 'ngoe ea liphoso tse kotsi ka ho fetisisa tsa aluminium alloy ingots. Ho hema hoa tšepe ho tla etsa hore ingot e be morao haholo kapa e se ke ea khoneha nakong ea ts'ebetso ea ho tiisa. E a phonyoha mme e teng ka ingot ka sebopeho sa hlephileng le masoba. Ka hona, ho nepahala ha ts'ebetso ea ho qhibiliha ha motsoako oa aluminium ho amana ka kotloloho le boleng ba ho qhibiliha. Ha e ame feela lik'hemik'hale tsa eona, empa e ama le boleng ba ingot esita le ea ho qetela Boleng ba lihlahisoa tse sebetsitsoeng bo amana haufi. Aluminium e sebetsa haholo, ntle le likhase tsa inert, e itšoara ka likhase tsohle.
Ho feta moo, liketso tsena ha li fetohe. Ha tšepe e se e sebelisitsoe, e ke ke ea fokotsoa, e leng se bakang tahlehelo ea tšepe. Ho feta moo, lihlahisoa (li-oxide, li-carbide, jj.) Tse kenang qhibilihisong li tla silafatsa tšepe ebe li baka litšitiso moahong o ka hare oa ingot. Ka hona, ts'ebetsong ea ho qhibiliha ea lits'ebetso tsa aluminium alloy, ho na le khetho e thata ea lisebelisoa tsa ts'ebetso (joalo ka mofuta oa sebopi, mokhoa oa ho futhumatsa, jj.), Le khetho e thata le mehato ea ts'ebetso ea ts'ebetso, joalo ka ho khutsufatsa nako ea ho qhibiliha le ho laola lebelo le nepahetseng la ho qhibiliha. Sebelisa ts'ebetsong ho koahela joalo-joalo.
- Ka lebaka la tšebetso ea aluminium, nakong ea mocheso o qhibilihisang, e tla sebetsana ka katleho le mongobo sepakapakeng le mongobo, oli, li-hydrocarbon, jj letotong la lits'ebetso. Ka lehlakoreng le leng, khase e qhibilihisitsoeng e ea eketseha, e baka ho hlepha le masoba, ka lehlakoreng le leng, sehlahisoa se ka silafatsa tšepe. Ka hona, mehato eohle e lokela ho nkuoa ho fokotsa mongobo nakong ea ts'ebetso ea ho qhibiliha, mme lisebelisoa tsa ts'ebetso, lisebelisoa le lisebelisoa tse tala li lokela ho bolokoa li omme le oli e silafalitsoe.
- Khamphani e sebelisa mokhoa o tsoelang pele oa ho qhibilihisa, mokhoa ona o iphepa o sa khaotse, 'me o tsoa hanyane ka hanyane. Bakeng sa ho qhibiliha ha motsoako oa aluminium, ka lebaka la sebopeho sa sebopi, nako ea bolulo ea ho qhibiliha e lokela ho ba e khuts'oane kamoo ho ka khonehang. Hobane nako ea bolulo ea ho qhibiliha e nka nako e telele, haholo-holo maemong a phahameng a qhibilihang, palo e kholo ea li-crystal nuclei tse sa sebetseng lia tima, li baka lithollo tsa kristale tse kenang haholo, tse bakang ho lahla litšila, le ho monya tšepe, ho etsa hore ho qhibiliha ho se metallic inclusions le The dikahare khase eketseha.
- Khase e sepakapakeng sebōping sa tšepe e qhibilihisang ke o mong oa mehloli ea bohlokoahali ea khase. Ho ipapisitse le mofuta le sebōpeho sa sebōpi se qhibilihisang se sebelisitsoeng, le mokhoa oa ho tuka kapa oa ho futhumatsa oa mafura a sebelisitsoeng, sepakapaka sa sebōpi hangata se na le boholo ba haedrojene (H2), oksijene (O2), mouoane oa metsi (H2O), carbon dioxide ( CO2), le carbon monoxide. (CO), naetrojene (N2), sebabole dioxide (SO2) ntle le li-hydrocarbon tse fapaneng. Liphetho tsena ehlile ha lia fella, 'me sebopeho sa tsona se pharalletse haholo. Lebaka ke hore sehlahisoa sa mollo o tsoang seboping sa sebōpi-sebōpi se fetoha haholo ebile ha sea tsitsa. Mona re kenyelletsa tšebetso ea ho kenella ha hydrogen (H) ka mokelikeli oa aluminium alloy, o kenyelletsang haholo lits'ebetso tse tharo: adsorption, diffusion, and dissolution.
Hobane haedrojene ke khase ea yuniti e nang le sebopeho se batlang se le bonolo, liathomo tsa eona kapa limolek'hule li nyane haholo, ho bonolo ho qhibiliha ka tšepe, mme ho bonolo ho hasana ka potlako maemong a batang haholo. Ka hona, hydrogen ke khase e qhibilihang habonolo ka tšepe.
Ts'ebetso ea ho qhibiliha ha haedrojene ka aluminium e qhibilihisitsoeng: adsorption ea 'mele- + adsorption ea lik'hemik'hale →> ho hasana
Hydrogen ha e sebetse ka lik'hemik'hale le aluminium empa e teng likheo tsa lekhoakhoa la kristale sebakeng sa ionic, e leng se etsang tharollo e tiileng ea mahareng. Ha ho se na filimi ea oxide ka holim'a tšepe ea mokelikeli, sekhahla sa khase se kenang ka tšepe se ts'oana hantle le botenya ba tšepe, bo lekana le motso o sekwere oa khatello ea khase, mme e eketseha ka mocheso o ntseng o eketseha
Moo: v phallo ea sekhahla n-metallic d-metal botenya E-activation eneji, le-p-khase khatello ea khatello ea R-khase khafetsa T-mocheso K Ka hona, pele o fihlela ho qhibiliha ha khase, mocheso o qhibilihisang o phahameng, ho arohana ha hydrogen Limolek'hule Ha lebelo le potlakile, lebelo le hasana ka potlako, ka hona, khase e phahama haholo.
Tlas'a maemo a tlhahiso, ho sa tsotelehe hore na ho sebelisoa sebopi sa ho qhibilihisa mofuta ofe ho hlahisa motsoako oa aluminium, ho qhibiliha ho amana ka kotloloho le moea, ke hore, le moea
Oxyjene e khase e kopana le naetrojene. Aluminium ke tšepe e batlang e sebetsa. Kamora hore e kopane le oksijene, e tla hlahisa oxidation e matla ho theha alumina.
Hang ha aluminium e entsoe oxidized, e fetoha slag e nang le oxidized mme e ba tahlehelo e ke keng ea etsolloa. Alumina ke ntho e tsitsitseng haholo, haeba e kopantsoe le ho qhibiliha, e tla fetoha slag e nang le oxidized. Ka lebaka la kamano e phahameng ea aluminium le oksijene, karabelo lipakeng tsa oksijene le aluminium e matla haholo. Leha ho le joalo, bokaholimo ba aluminium bo sebetsa ka oksijene ho hlahisa Al2O3, 'me bophahamo ba molek'hule ea Al2O bo boholo ho feta ba aluminium, ka hona lera la aluminium le na le oxidized ho theha A12O; filimi e teteaneng, e ka thibelang liathomo tsa oksijene hore li se ke tsa hasana ka hare ka har'a filimi ea oxide Ka nako e ts'oanang, e ka thibela li-ion tsa aluminium hore li se ke tsa hasana ka ntle, ka hona ea thibela ho kenella ha aluminium ho ea pele.
Phekolo ea Aluminium Alloy
Kalafo ea motsoako oa aluminium haholoholo e kenyelletsa ho tlosoa ha slag le ho hloekisoa.
- (1) Ka tshebetso ya ho slagging aluminium motsoako qhibiliha, ka lebaka la sa sebetse slag tloswa le tlhoekiso, e nyenyane slag e qhibiliha ka qhibiliha, fella ka sebopeho sa matheba a lehloa holim'a motsoako oa aluminium, e leng ka ho teba ama boleng ba motsoako oa aluminium. Haeba ho tlosoa ha slag ho sa hloeka, Ho tla baka li-slag inclusions le maraba a mang, mme ho lahla ho tla hlakoloa. Aluminium ke mofuta oa tšepe e sebetsang. Ho bonolo ho hlahisa li-oxide tsa aluminium nakong ea ts'ebetso ea ho qhibilihisa. Tse ling tsa inclusions tseo e seng tsa tšepe le tsona li bonolo ho kena qhibiliha. Li-inclusions li kotsi haholo ho lihlahisoa tsa aluminium. Ho tlosoa ha inclusions e bile mosebetsi o ka sehloohong oa tlhoekiso ea aluminium e qhibilihisang. Ts'ebetsong ea tlhahiso, li-inclusions tse tloaelehileng tsa aluminium alts lia qhibiliha ke Al203, SiO2, MgO, jj. E tla baka ho se hloeke ha tšepe e qhibilihisitsoeng, li-inclusions li tla ama ho qhibiliha ho qhibilihang, ho fetoloa ha matla ho tla hlahisa bubble nakong ea ts'ebetso ea ho tiisa, e tla ama boemo ba ho nyenyefala. Hobane bongata ba likaroloana tsa oxide e ntle li ts'oana le tsa aluminium, hangata li emisitsoe ka aluminium e qhibilihisitsoeng, mme ho thata ho li tlosa ka ho ema. Hangata oxide e tlositsoeng e na le aluminium e ngata. Le ha ts'ebetsong e na le lits'ebetso tse ling tse ngata, ho fokotsa ho kenella ha aluminium le ho tlosa inclusions tse nang le oxidized ke mabaka a mantlha a ho sebelisa ts'ebetsong. slag le metsi, 'me u hule slag e arohaneng ka seboping, hobane moemeli oa slagging o na le NajAIF. (Kapa KzSiFg), letsoai lena le na le bokhoni ba ho hlahisa adsorb Al2O3, hammoho le Na2SiF. Karabelo ea pele e ka ja karolo ea Al2O3, mme karabelo ea boraro e arola slag le metsi, 'me e hula slag ka seboping ho fihlela Morero oa ho tlosoa ha slag. Ka nako e ts'oanang, e hlahisa NaAlF%, e nang le phello ea ho hlahisa adsorbing ka matla r-Al2O3, ho etsa slag le aluminium Mokelikeli o arohane. Morero oa ts'ebetso ea slag ea ho tlosa aluminium ke ho tlosa litšila le slag ea oxide e kenang aluminium e qhibilihisitsoeng. Khafetsa slag e na le aluminium e qhibilihisitsoeng nakong ea ho tlosoa ha slag. Ka hona, ho na le tšepo ea hore aluminium e qhibilihisitsoeng e ka har'a slag e lokela ho ba hanyane ka moo ho ka khonehang, mme slag e lokela ho qhekelloa hape. Morero oa ho monya molora ke ho pepeta aluminium e qhibilihisitsoeng ka slag ebe e teba botlaaseng ba moahi, e le hore slag e robehe butle mme e qhalane karolong e kaholimo, e le hore slag le aluminium e qhibilihisitsoeng e arohane. Ho fihlela sena, slag e ntle e tlosang ts'ebetsong e tlameha ho khethoa. . Mokhoa oa ho tlosoa ha slag o ipapisitse le palo ea aluminium e qhibilihisitsoeng seboping sa ho qhibilihisa, ka mokhoa o ts'oanang o kenya sesebelisoa sa slag ho latela palo e hlokahalang, ebe o hlohlelletsa ka lebelo le sa fetoheng, ebe o ntša sefahleho sa slag kamora ho ema bakeng sa 8- Metsotso e 10. The slagging hloka hore mocheso oa aluminium entsoeng ka ho qhibilihisoa ho ba 720-740C.
- (2) Ho hloekisa: Lik'hemik'hale tsa aluminium li sebetsa ka makhetlo a 17. Ka hona, le ha haedrojene e ka mokelikeling oa alloy e le tlase haholo, bongata bo bongata ba haedrojene bo tla kenella nakong ea ho tiisa, ho etsa li-pinholes le inclusions ho li-castings, tse tla ama ka botebo thepa ea mochini oa aluminium alloy. Ho ntlafatsa boleng ba aluminium alloy ho qhibiliha le ho hloekisa mokelikeli oa motsoako ke e 'ngoe ea lintlha tsa bohlokoa ho qhibilihisoa ha motsoako oa aluminium, hape ke tsela e atlehang le mekhoa ea ho ntlafatsa boleng ba sehlahisoa le tlholisano ea mmaraka ea li-castings tsa aluminium. Ts'ebetso e sa utloahaleng ea ho hloekisa, alloy degassing ha e hloeke, li-castings li tloaetse ho ba masoba. Bakeng sa ho eketsa litlamorao tsa ts'ebetso, ho bohlokoa ho eketsa palo ea moemeli oa ho hloekisa. Leha ho le joalo, haeba palo e le ngata haholo, ho bonolo ho baka ho chesoa ha oxidation ea Mg. Al, Ti le likarolo tse ling, le sebopeho sa slag ea oxidation. Bakeng sa sena-ts'ebetso ea bohlokoa ea ho hloekisa alloyum alloy e bohlokoa. Boithuto bo bonts'itse hore bokhutšoaane ba sebaka se hlokahalang bakeng sa haedrojene ho fihlella bubble, lebelo la degassing le potlakile. Khamphani ea rona e khethile mochini oa rotor deaerator o ntlafalitsoeng ke FOSECO bakeng sa phokotso ea mokelikeli oa aluminium alloy. Molao-motheo oa eona o sebetsang ke hore: male rotor e potolohang e roba matšoafo a maholo a khase e tloaelehileng ea inert ebe e a hasanya ka tšepe e qhibilihisitsoeng. Ka ho fokotsa bophara ba bubble, bokaholimo ba bubble bo eketseha haholo, mme ho na le ho hloka matla ho hoholo. Bokaholimo ba bubble bo kopane le haedrojene le litšila ka tšepe e qhibilihisitsoeng, ka tsela eo li ntlafatsa ts'ebetso ea ts'ebetso. Rotating degassing e potolohang e amoheloa e le e 'ngoe ea lits'ebetso tse ntle ka ho fetesisa. Sebopeho setshwantsho sa mochine o potolohang oa rotor degassing ke: enjene e khanna molamu o potolohang le graphite rotor ho potoloha, mme khase ea inert e kenella molamu o potolohang ka ho kopanya ho potoloha. Lere le potolohang le graphite li na le lesoba le bohareng le lumellang khase e kenang hore e fete ebe e fafatsa ka mokelikeli oa tšepe. Rotor e potolohang e qhaqha makhapetla a khase a kenang ka hare ho li-bubble tse ntle haholo, tse hasaneng ho pholletsa le tšepe e qhibilihisitsoeng. Ka ho fetola le ho laola sekhahla sa phallo ea khase e kenang le lebelo la graphite rotor, boholo ba bubble bo laoloa mme ts'ebetso ea tlhoekiso ea ntlafatsoa. Ka nako e ts'oanang, moemeli oa ho hloekisa o behiloeng mochining oa degassing o eketsoa mokelikeli oa aluminium o sebetsitsoeng ka karolo e itseng ho netefatsa hore scum ea oxide e tlosoa hape nakong ea ts'ebetso. Ho hloekisa litlhoko tsa ts'ebetso: fetisetsa metsi a aluminium ka sebōping sa ho qhibilihisa ho deaerator e nang le mokotla oa metsi oa phetisetso: khatello ea naetrojene e hlokang ho laoloa ho 0.1-0.3mpa ho thibela aluminium hore e se ke ea phatloha le ho utloisa bohloko; Nako ea ho hloekisa le ho laola e laoloang nakong ea 5min. Ho tlosoa ha slag le ho hloekisoa ha motsoako oa aluminium ea die-cast ke ts'ebetso ea nako, e ke keng ea phetheloa kapele. Ke ts'ebetso e fosahetseng ho khutsufatsa nako ea ho hloekisa. Ho tšeloa ha khase ka har'a aluminium e qhibilihisitsoeng le ho phaphamala ha litšila ho hloka nako e lekantsoeng, feela tiiso Ho na le nako e lekaneng ea adsorption le nako ea ho se hloeke e phallang ho fihlela sepheo sa ho hloekisa. Nakong ea ho hloekisa, etsa bonnete ba hore mokelikeli oa aluminium o kopane ka botlalo le bubble. Khathatso ea kamehla ea hlokahala. Khase e mokelikeli oa aluminium ea tlosoa ebe ho tlosoa litšila ho netefatsa li-pores tsa sehlahisoa.
5.Conclusion
Ho khetha ts'ebetso e nepahetseng ea ho qhibilihisa molemong oa tlhahiso ea sesebelisoa sa aluminium ke mohato oa pele oa ho fumana boleng bo phahameng ba sehlahisoa. Taolo e thata ea lisebelisoa tse tala ke mohato oa bohlokoa oa ho qhibilihisa. Ka nako e ts'oanang, ho hlokahala hore o be le kutloisiso e bonolo ea litlamorao tsa likarolo tse fapaneng tsa alloy pele o qhibilihisoa. Ho tlosoa ha slag le ho hloekisa ke lits'ebetso tsa bohlokoa haholo ts'ebetsong ea ho qhibilihisa li-alloys tsa aluminium. Ka lipatlisiso tsa khopolo mabapi le ho tlosoa ha slag le degassing, ho fumanoe ts'ebetso e nepahetseng ea ho qhibilihisa k'hamphani ea rona.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape:Ho qhibiliha le kalafo ea ADC12
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off