Mocheso Phekolo Process Of High a mankanese le Low nikele Stainless Steel
Lilemong tsa morao tjena, ka tsoelo-pele e potlakileng ea moruo oa Chaena, tlhokahalo ea tšepe e sa hloekang e ntse e eketseha, 'me tlhokahalo e matla e tsamaisitse katoloso e potlakileng ea matla a tlhahiso ea tšepe ea China. Empa ka nako e ts'oanang, Chaena ke naha e haelloang ke lisebelisoa tsa nickel le chromium, kahoo ho bohlokoa haholo ho nts'etsapele le ho hlahisa tšepe e bolokang chelete e bolokang nickel. 1Mn5Cr10NiMo tšepe ke tšepe e tlase ea nickel martensitic e nang le Mn e nkang sebaka sa Ni. Tšepe ena e ka sebelisoa libakeng tseo ho hanyetsa ha kutu ho seng holimo haholo. Boithuto bo hlophisitsoeng haholoanyane ba ts'ebetso ea kalafo ea mocheso, ho thatafala le sebopeho sa tšepe ho na le bohlokoa ba tataiso bakeng sa ts'ebetso le ts'ebeliso ea eona hamorao.
Tšepe ea teko ke mohala oa tšepe oa 1Mn5Cr10NiMo o fumanoang ka ho phunya le ho bata ka mor'a ho qhibiliha li-ingots tse nang le sebopi sa motlakase + VOD + ts'ebetso ea ho hloekisa ka ntle, bophara ba Φ46mm, ka mor'a ho kenngoa, mohaho o halefile ka martensite, ts'ebetso ea annealing ke 820 ℃ × 20h serame, Fur. boima ba 360~385HB, metsoako ea eona ea lik'hemik'hale e bontšoa ho Lethathamo la 1. Ka mor'a ho kenngoa ha mocheso o phahameng o tloaelehileng, tšepe e na le boima bo phahameng, bo bakang mathata a maholo bakeng sa ho khaola laser Tshebetso.
Nka mehlala ea mekoallo e koetsoeng e batang bakeng sa ho tima le ho futhumatsa ho ithuta liphetoho bothateng ba tsona, sebopeho le thepa ea bona. Ts'ebetso e ikhethileng e tjena:
- Khetha lihlopha tse 9 tsa mehlala ho 1050 ~ 350 ℃, khetha lintlha tse 9 tsa mocheso oa 1h, ebe u li tima. Ka liphetoho ho thatafala le sebopeho, mocheso o boima oa phetoho ea mohato o ikemiselitse.
- Mocheso oa phetoho ea maemo a mahlonoko o khethiloeng ke mohato ① o khethiloe. Lihlopha tse hlano tsa mehlala li bolokiloe ho 960 ℃ bakeng sa 1h ebe li pholile moea. Li bolokiloe ho 750 ~ 580 ℃ bakeng sa 2h ebe li pholisoa le sebopi bakeng sa ho halefa ho ithuta liphetoho tsa bona tsa ho thatafala le thepa ea mochini.
Phello e bontša:
- Ar1 ea 1Mn5Cr10NiMo tšepe e ka ba 750 ℃, 'me Ar3 ke 900 ℃. Ha ho nahanoa ka tšusumetso ea superheat, ha e le hantle e lumellana le liphetho tsa lipalo tsa foromo ea bohlokoa ea ho bala mocheso oa tšepe ea hypoeutectoid. Ar1 le Ar3 li batla li le 20 tlase ho Ac1 le Ac3 ℃.
- Nakong ea tempering, ho na le ho thatafala ha sekhahla karolong e phahameng ea mocheso (> 630 ℃), mme thatafalo ea eketseha ka keketseho ea mocheso oa tempering. Ho thatafala ha bobeli ho bakoa haholo ke ho matlafatsoa ha li-carbide tse sa sisinyeheng, ho ntlafatsang matla a tšepe ka nako e le 'ngoe, Thatafalo le eona ea eketseha.
- Ho tloha ts'ebetsong e akaretsang ea matla a matla le ts'ebetso ea ts'ebetso, ho itšireletsa haufi le 690 ℃ ho na le matla a phahameng ka ho fetisisa le ts'ebetso ea ts'ebetso, mme thatafalo e ka ba 302HBW. Likarolo tse bohale tse ka tlase ho 600 ° C li na le kotsi ea ho robeha habonolo, ka hona mocheso o futhumetseng o lokela ho ba kaholimo ho 600 ° C.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape:Mocheso Phekolo Process Of High a mankanese le Low nikele Stainless Steel
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off