Ts'ebetso e Phahameng ea ho Itšireletsa ea Cold Wear Resistant Cold Work
Tšepe e phahameng e sa keneleng mosebetsi o batang e na le tšepe e phahameng ea chromium, limaraka tsa tšepe tse emelang ke: Cr12, Cr12MoV, Cr12Mo1V1, Cr12W, Cr12V, LD (7Cr7Mo2V2Si), ER5 (Cr8MoWV3Si), GM (9Cr6-W3Mo2V2) joalo-joalo. .
Boholo ba litšepe tse kaholimo ke litšepe tsa ledeburite. Ho na le palo e kholo ea li-carbides tsa eutectic ka sebopeho. Ho na le palo e kholo ea li-carbide tsa eutectic kamora ho tima lephaka. Khanyetso ea ho tsofala e phahame mme matla a ho jara a maholo. E atisa ho sebelisoa bakeng sa ho etsa thepa tlas'a maemo a phahameng qhoaele hanyetsa. Shoela ho sebetsa ho bata.
Khetho e nepahetseng ea kalafo ea mocheso oa thepa ke senotlolo sa tlhahiso ea tšebetso. Ke entse mochini o theolang moea o tlase le o khutlisetsang tlaase le lipalo-palo tse khopamisang kalafo ea mocheso oa sehlahla se nang le joala se sebelisang polyvinyl alcohol (PVA) slurry. Sehloohong sena, sehlahla se behang se sebetsa ho polyester (PET) slurry, 'me mocheso oa ts'ebeliso o phahame, ho 350 ℃ Hoo e ka bang, e phahameng ho feta mocheso oa ts'ebeliso oa PVA slurry (e ka bang 100 ℃), ho beha ho reretsoe ho amohela Ho tima le ts'ebetso e phahameng ea kalafo ea mocheso.
Mekhoa ea ts'ebetso ea sehlahla se behang e koala → ho theha → ho koala sekhahla → ho betla → ho tima lephaka → ho sila, jj. Teko ena e shebile le ho lekola ts'oaetso ea microstructure, thatafalo le kalafo ea mocheso oa sehlahla se jereng kamora ho koala le ho tima ho phahameng. le ts'ebetso e phahameng ea ho hlaphoheloa, e le ho fana ka liphetoho tsa nako e tlang bakeng sa mofuta ona oa thepa le kabelo ea boholo ba thepa pele e tima. tshupiso.
Hajoale, kalafo ea mocheso oa thepa ea Cr12 e ikarabella ho feta 50% ea matla a ho sebetsa a hlobo e batang ea mosebetsi. Ho tseba mekhoa e fapaneng ea kalafo ea mocheso, litšobotsi tsa microstructure le melao e sothehileng ea lisebelisoa tsena e na le bohlokoa bo tataisang bakeng sa tlhahiso ea hlobo ea lipatlisiso tsa saense le tlhahiso.
Cr12MoV tšepe e behang sehlahla ke mofuta oa karolo e jereng e sebelisoang lik'hemik'hale, mechini le liindastering tse ling. E sebetsa tlas'a khatello e itseng, mocheso le mahareng. Maemo a ts'ebetso a thata ebile ts'ebetso ea tlhahiso e rarahane. Ntle le ho boloka thatafalo e phahameng tlasa maemo a itseng a mocheso, tšepe ea Cr12MoV ea ho etsa lihlahla tse nang le lihlahla e tlameha ho ba le ts'ireletso, ts'ireletso ea ts'enyeho, ho hanyetsa oxidation, botsitso bo botle ba 'mele le quilting e ntle. Processing tshebetso, joalo-joalo
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape: Ts'ebetso e Phahameng ea ho Itšireletsa ea Cold Wear Resistant Cold Work
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off