Hlobo Mocheso Phekolo Bokaholimo Matlafatsa And Phetolo Technology
Theknoloji e matlafatsang bokhabane
1) hlobo thunngoa peening le mosebetsi oa eona
Ts'ebetso ea ho thunya ke mokhoa oo ho oona ho fafatsoang palo e kholo ea li-projectile bokaholimo ba karolo, mme projectile e fafatsoa ka holim'a karolo joalo ka ha eka lihamore tse nyane tse nyane li hamore bokaholimo. Ka hona, bokaholimo ba karolo ea tšepe bo hlahisa deformation e matla haholo ea polasetiki, e etsang hore bokaholimo ba hlobo bo hlahise botenya bo itseng. Lera le thatafatsang mosebetsi le bitsoa mochini o matlafatsang bokaholimo. Lera lena le matlafatsang le tla ntlafatsa haholo mokhathala oa likarolo tse tlas'a mocheso o phahameng le maemo a phahameng a khatello ea maikutlo.
2) Bokaholimo phetoho ea ho thunngoa ho qhomisa e cavity
- (1) Matšoenyeho a setseng a macro.
- (2) Matšoenyeho a microscopic a bokaholimo ba bokaholimo.
- (3) Sebopeho se setle sa mosaic sa lera le kaholimo.
3) Shot peening mochini le thunngoa peening tshebetso entsprechen
Shot mechine ho qhomisa e arotsoe pneumatici thunngoa ho qhomisa e mechine le centrifugal thunngoa ho qhomisa e mechine. Pneumatici thunngoa ho qhomisa e mochini ke hore ha a petetswa moea fuoa ke konpresser moea e feta ka sethunya spray, khatello mpe etsa hore projectile ho anya batho le tsoe nozzle ka lebelo le phahameng, eaba ba etsa bokaholimo ba karolo e moo projectile molapo e nyanyatsoa. Ho boetse ho na le mochini oa ho tsamaisa likarolo mochini oa ho thunya, o ka netefatsang ho ts'oana ha peeling le ho koahela ho itseng. Shining peening haholo-holo e hloka ho laola matla a ho thunya. Ho na le matla a itseng a ho thunya bakeng sa boemo bofe kapa bofe ba ts'ebetso ea ho thunya, empa ho tseba matla a ho thunya, ho tlameha ho lekanngoa bolelele ba arc.
2.Phetoho ea theknoloji ea ho roala hlobo
1) Mokhoa o thata oa ho roala chromium o maemong a bohlokoa ho matlafatseng hlobo e itseng.
Ho na le melemo ea ho barbotage coefficient tlaase barbotage, phahameng thatafala (ka 1100HV), kopo e bonolo, 'me a pheta mochini oa cnc. Leha ho le joalo, hoa lokela ho hlokomeloa hore haeba botenya ba seaparo bo khethoa ka mokhoa o sa utloahaleng, bo tla baka tšenyo pele ho nako hlobo. Ha hlobo e le tlas'a khatello e matla kapa tšusumetso, ho roala ho bonolo ho eboloa, ho baka tšenyo pele ho nako hlobo. Ka hona, seretse se thata sa chrome se ke ke sa sebelisoa bakeng sa lihlooho tse batang tse shoang le ho se na letho hoa shoa. E loketse feela ho khumama le ho etsa lisosa ka khatello ea maikutlo e tlase.
2) Nickel-phosphorus alloy e koahetsoe
Mosebetsi o etselitsoeng pele o kentsoe ka har'a tharollo e nang le letsoai la nikele, ho fokotsa moemeli le lisebelisoa tse ling, mme karabelo ea ho fokotsa li-autocatalytic e tla hlaha holim'a setsi sa mosebetsi, ho fokotsa li-nickel tharollong ea tšepe le ho beha holim'a metsi. workpiece (hlobo) Theha mokato.
3) Phallo ea mouoane ea lik'hemik'hale
Mokhoa oa ho roala bokaholimo ho latela molao-motheo oa phepelo ea lik'hemik'hale o bitsoa phepelo ea lik'hemik'hale, kapa CVD ka bokhutšoanyane. Likarolo tse sebetsang tsa hlobo tse hlokang ho kenella li futhumetse ho isa ho 1000 ° C ka lephaka, ebe li lebisa ho TiCl4, H2, CH4 le likhase tse ling tse sebetsang. Ha khase e kopana le mocheso o phahameng o sebetsang holim'a metsi, e ka hlahisa TiN, TiC le metsoako e meng tlasa ts'ebetso ea mocheso o phahameng. E khomarela ka tieo bokaholimo ba likarolo tsa hlobo ho etsa seaparo se thata haholo.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape: Hlobo Mocheso Phekolo Bokaholimo Matlafatsa And Phetolo Technology
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off