Lipatlisiso ka Sebopeho le Ts'ebetso ea Low Pressure Casting Aluminium Alloy Rear Sub Frame
Ha lefatše le ntse le lebisa tlhokomelo e eketsehileng bothateng ba tšilafalo ea tikoloho, lik'hamphani tsa likoloi li entse lipatlisiso le nts'etsopele ea lisebelisoa tse ncha le mahlale a morao-rao a bobebe, 'me koloi e bobebe e fetohile tataiso ea bohlokoa ea nts'etsopele. Boithuto bo bontšitse hore 60% ea ts'ebeliso ea matla a koloi e tsoa boima ba koloi. Ha boima ba lisebelisoa tsa makoloi bo fokotsoa ka 10%, ts'ebeliso e ts'oanang ea mafura e ka fokotsoa ka 6% ho isa ho 8%. Ka nako e ts'oanang, bobebe bo ka ntlafatsa ts'ebetso ea braking ea likoloi ho isa bohōleng bo itseng, ea etsa hore likoloi e be lipalamo tse sireletsehileng, tse mabothobotho hape tse mosa tikolohong. Lisebelisoa tsa aluminium alloy li fetohile khetho ea pele bakeng sa likoloi tse bobebe kajeno ka lebaka la boima ba tsona bo bobebe, matla a ikhethileng a phahameng, ts'ebetso e bonolo, le ts'ireletso e ntle ea ts'enyeho.
E le karolo ea bohlokoa ea sebopeho sa cheisi ea koloi, subframe e ka morao e bapala karolo ea ho ts'ehetsa li-axles tse ka pele le tse ka morao le ho emisa, tse ka ntlafatsang taolo ea ho khanna haholo, ho palama polokeho le boiketlo. Ka nako e ts'oanang, phokotso ea boima ba subframe e ka morao e ka ntlafatsa kakaretso Ts'ebetso e jereng mojaro oa koloi e bohlokoa haholo ho ntlafatseng ts'ebetso le botsitso ba koloi. Ka hona, khetho ea lisebelisoa tsa subframe e ka morao e bohlokoa haholo ntlafatsong ea ts'ebetso ea koloi eohle. Mefuta e mengata ea morao-rao ea morao-rao e entsoe ka lipoleiti tsa tšepe, 'me ke mefuta e fokolang feela e sebelisang li-subframes tsa aluminium alloy.
Sebopeho se ka morao sa subframe ea mofuta o itseng oa Zotye Automobile o amohela lisebelisoa tsa aluminium alloy. Ka moralo o utloahalang oa moaho le ts'ebetso e hlophisehileng, khatello e tlase e nang le khatello e tlase e sebelisetsoa ho fumana subframe e ka morao e fihlellang litlhokahalo tsa matla le botsitso, mme e ntlafatsa khanya ea koloi. Boemo ba quantification. Subframe e ka morao e na le boholo ba kantle ba 1 165 mm × 798 mm × 396 mm, botenya bo boholo ba lebota ba 5 mm, le boima ba 30.5 kg. Ke karolo e kholo le e rarahaneng ea marako a tšesaane a nang le matla a phahameng, ho ba thata haholo le ho hanyetsa kutu, le likarolo tsa tšepe. Ha e bapisoa, e ka fihlela phokotso ea boima ba lik'hilograma tse 10.1, 'me sekhahla sa phokotso ea boima e ka ba 33%.
Lits'ebetso tsa mochini oa lits'epe tse kopantsoeng tsa aluminium li ipapisitse le litšobotsi, kabo le tlhaho, palo le boholo ba liphoso tsa karolo ea bobeli. Liphoso tsa microscopic ke mohloli oa mapetso a fracture ea aluminium alloy mme li na le tšusumetso e kholo ho thepa ea mochini. Ka hona, ho hlokahala hore ho hlahlojoe microstructure le thepa ea mochini oa khatello e tlase ea khatello ea aluminium alloy subframe e sebelisitsoeng ka katleho.
Teko ea benche ea ho tšoarella
Sistimi ea teko ea mokhathala e mene e sebelisitsoe ho etsisa likarolo tsa foreimi e ka morao. Kamora liteko tse 300,000, bokaholimo ba sehlahisoa bo ne bo se na liphoso tse kang mapetso mme bo fetisitse tlhahlobo ea ho tšoarella. E bonts'a hore ts'ebetso ea sekhahla se tlase kamora ho lahla khatello e tlase e fihlela litlhoko tsa moralo, mme cheisi e bobebe e ntlafalitsoe.
Teko ea ho tšoarella tseleng ea koloi eohle
Karolo e ka morao e ka morao e na le koloi eohle, 'me ho etsoa teko e felletseng ea ho tšoarella ea 30,000 km ho Yancheng Proving Ground ho netefatsa ho tiea ha likarolo tsa foreimi e ka morao. Liphetho li bonts'a hore ts'ebetso ea subframe e ka morao e fihlela litlhoko tse tloaelehileng.
fihlela qeto e
- Sesebelisoa sa morao-rao sa khatello ea aluminium se nang le khatello e tlase se na le thepa e ntlehali ea mmuso oa T6, ka matla a ho tensile a 304 MPa, matla a karolelano ea lihlahisoa tse 245 MPa, karolelano ea bolelele ba 8.2%, le boima ba karolelano ea (HBW) ea 99HB, Ho fihlela litlhoko tsa moralo oa potlana ea foreimi.
- Ponahalo ea sekhahla se tlase kamora khatello e tlase ea aluminium ha e na liphoso tse hlakileng, sebopeho sa kahare se teteaneng, eutectic Si ke elliptical e putsoa e ajoang ho α-Al matrix, le palo e nyane ea tšepe e tšoeu e khanyang motsoako o ajoa moeling oa lijo-thollo ka sebopeho sa masapo.
- Karolo e thata ea sekhahla sa ZL101A-T6 e na le palo e kholo ea li-dimples tse lekanang le palo e nyane ea libaka tsa quasi-cleavage, 'me mokhoa oa ho robeha ke ho robeha ho kopaneng ha ductility le brittleness.
- Sesebelisoa sa morao-rao se nang le khatello e tlase ea aluminium se atlehile ho fetisa tlhahlobo ea benche e tšoarellang le teko ea ho tšoarella tseleng ea koloi, mme ts'ebetso ea eona e fihletse litlhokahalo tsa moralo.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape:Lipatlisiso ka Sebopeho le Ts'ebetso ea Low Pressure Casting Aluminium Alloy Rear Sub Frame
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off