Mehato ea ho fokotsa likahare tsa haedrojene, oksijene le naetrojene ka tšepe
Ka kakaretso, tšepe e hloekileng e bua ka sehlopha sa tšepe se nang le lintlha tse tlase tsa likarolo tse hlano tsa ho se hloeke (S, P, H, O, N) ka tšepe, 'me e laola ka thata li-inclusions tse seng tsa tšepe (oxides, sulfides) ka tšepe. Mehato e akaretsang ea ho fokotsa likahare tsa [H], [O] le [N] ka tšepe e kenyelletsa:
1, [H] litaba
(1) Ho tlosa moea o hloekileng
"Ho fokotsa PH2 ho ka fokotsa ho qhibiliha ha haedrojene ka tšepe, ka hona, vacuum degassing e ka sebelisoa ho fokotsa likahare tsa [H] ka tšepe.
(2) Fokotsa mongobo oa thepa
80% ea haedrojene e entsoeng ka tšepe e qhibilihisitsoeng e tsoa lisebelisuoa tse tala, thepa e hanyetsang le mongobo sepakapakeng. Tlhokomelo e lokela ho fuoa ho baka ha ladle, tundish, ferroalloy, lisebelisoa tse thusang, haholo-holo kalaka.
Ntle le moo, khokahano e tobileng ea tšepe e qhibilihisitsoeng le sepakapaka e lokela ho fokotsoa: tšepe e qhibilihisitsoeng kamora kalafo ea lephaka e lokela ho qoba ho matlafala hape, 'me khatello ea argon e lokela ho laoloa ho thibela tšepe e qhibilihisitsoeng hore e se ke ea pepesetsoa; ka nako e ts'oanang, ts'ireletso e lokela ho etsoa nakong ea ho tšela.
2, [N] litaba tse ka hare
e ts'oana le mokhoa oa ho fokotsa [N] litaba tsa tšepe. Taolong ea ho fokotsa likahare tsa [N] ka tšepe, ntle le kalafo e hloekisang ea tšepe e qhibilihisitsoeng le ho fokotsa puisano ea tšepe e qhibilihisitsoeng le sepakapaka, ho tsepamisitsoe maikutlo taolong ea lisebelisoa tsa alloy.
Nakong ea ts'ebetso, likarolo tse fokotsang boleng ba naetrojene ka tšepe (Si, Ni) li eketsoa ho fihla moeling o kaholimo oa sebopeho, mme likarolo tse eketsang boleng ba naetrojene ka tšepe (Mn, Cr, Mo, V, Nb) lia laoloa sebakeng se itseng ho fokotsa litlamorao tsa Eona tse mpe.
3, [O] litaba
(1) Tlhoekiso ea sebopi sa tšepe e qhibilihisitsoeng
Ts'ebetso ea ho hloekisa e ka tlosa lipalo tse ka bang 80% tsa tšepe e qhibilihisitsoeng.
(2) Ntlafatsa ho nepahala ha taolo ea litaba tsa C pheletsong ea sebopi sa motlakase
Leka ho ntlafatsa pheletso ea taolo ea ntlha ha u letsa oksijene seboping sa motlakase ho fokotsa ho feta.
(3) Thibela ho qhekelloa
Theknoloji ea slag e phallang pele e tlanya, ho tlanya ka tlase le tšepe e qhibilihisitsoeng e lekaneng seboping ho amoheloa ho thibela ho ts'oaroa.
(4) Taolo ea Deoxidizer
K. Taelo e utloahalang ea ho kenela. Taelo ea ho eketsa deoxidizer ke e latelang: pele u tlanya, eketsa Fe-Mn e nyane ka har'a ladle, eketsa Fe-Si kamora ho tlanya, 'me u sebelise sesebelisoa sa terata ho fepa Al ha u hloekisa kantle ho seteishene sa ho hloekisa.
B. Karolelano e nepahetseng ea Mn / Si. Ha Mn / Si> 2.5, MnO-SiO2 e tloaelehileng e theoa mme e phahama habonolo.
C. Mefuta e loketseng ea Al. Ha [Al] = 00.01-0.02%, T [O] e tsamaellanang ke eona e tlase ka ho fetisisa.
D, deoxygenation ea hoqetela. Bakeng sa ho matlafatsa ts'oaetso, Si-Ca e sebelisetsoa ho felloa ke matla kamora ho hloekisa.
(5) Laola hantle slag
Laola sebopeho sa slag, mocheso le slag ho ntlafatsa bokhoni ba inclusions ba ho qhala sehlopheng sa slag.
(6) Loketseng susumetsang matla
Ho tsukutleha ho loketseng ho sebelisetsoa ho hatisa hore inclusions e ka tlosoa ntle le ho kenyelletsa slag ea tšepe ka tšepe e qhibilihisitsoeng. Ntle le moo, ho thunya ho bonolo ho ka sebelisoa pele ho hloekisoa.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape: Mehato ea ho fokotsa likahare tsa haedrojene, oksijene le naetrojene ka tšepe
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off