Litaba li hloka tlhokomelo ha ho raloa sebopeho sa ho lahla
Kaha ho lahla hoa bata ebile ho tiisa ka potlako ka hlobo ea tšepe ho feta hlobo ea lehlabathe, 'me hlobo ea tšepe ha e na mamello, ha hlobo ea tšepe e lahleloa, khatello ea kelello e hlahisoang ha e betloa e kholo ho feta ea ho betloa ha lehlabathe. Liphoso tse kang ho tšolla ho sa lekanang, mokoallo o batang, molomo o mosoeu (bakeng sa ho betloa) joalo-joalo hangata:
Tlhokomelo e lokela ho fuoa lintlha tse latelang tsa sebopeho ho thibela mapetso a litšepe tsa tšepe:
- K. Litlhokahalo tsa botenya ba lerako le ts'oanang, phetoho e bonolo le khokahano lipakeng tsa mabota, lesela le nepahetseng likhutlong, jj e lokela ho ba thata ho feta ho lahla lehlabathe;
- B Mabota a hoketsoeng ka nqa e le ngoe a lokela ho fetoloa hore a hokahane hantle;
- C Likarolo tse fokolang tsa sebopeho li lokela ho matlafatsoa ka likhopo, li-boss, jj ho thibela ho lahla mapetso;
- D Leka ho fokotsa li-protrusions, likhopo, li-flanges le likarolo tse ling tse hlahelang tse sitisang ho fokotseha ha mahala;
- Ha o hlophisa khopo e matlafatsang ho laoleng, tšusumetso ea eona ho shrinkage ea ho betsa le eona e lokela ho tsotelloa.
Tlhokomelo e lokela ho fuoa mathata a latelang a sebopeho ho thibela ho ts'ela ho lekaneng le ho itšehla thajana ha litšepe tsa tšepe:
- K. Botenya ba lebota bo lokela ho ba bo loketseng eseng bo bosesane haholo, haholoholo ha boholo ba samente bo le boholo;
- B. Sebaka se seholo se rapameng se lokela ho qojoa, hobane se etsa hore tšepe e qhibilihisitsoeng e nyolohe butle haholo nakong ea ho betsa, mme bokaholimo bo kopaneng le moea bo boholo, bo bonolo ho bo kopanya. Ka nako e ts'oanang, ka lebaka la mocheso o potlakileng oa mocheso oa tšepe, tšepe e qhibilihisitsoeng e lahleheloa ke metsi ka potlako 'me ho bonolo ho e baka. Ho se lekane, mokoallo o batang, kenyelletso ea slag le liphoso tse ling;
- C. Sebopeho sa ho betsa se lokela ho hlophisoa ka hohle kamoo ho ka khonehang ho qoba likarolo tse bohale le likhutlo le likhokahano tse fetohang haholo ho tsamaisa phallo ea tšepe e qhibilihisitsoeng.
Ha u rala li-castings tsa tšepe tse nang le libopeho tse rarahaneng haholoanyane, haeba ts'ebetso ea tlhahiso e na le mathata a maholo, leka ho etsa hore castings e be bonolo ka chebahalo le sebopeho se matla se fetohe ntle le ho ama maemo a ts'ebeliso ea li-castings ho thusa ho tlosoa ha castings ho tloha hlobo ea tšepe.
Ha ho raloa likarolo tsa mantlha tsa sebopeho sa tšepe le ho khetha mekhahlelo ea tsona, hangata ho hlokahala ho ela hloko:
- (1) Ka lebaka la mocheso o potlakileng oa hlobo ea tšepe, botenya ba lebota la tšepe bo lokela ho ba kholo ho feta ba ho betsa lehlabathe;
- (2) Botenya ba lebota le kahare le khopo e kahare ea ho betsa e lokela ho ba 0.6-0.7 ea botenya ba lebota le kantle le kopaneng, ho seng joalo lebota le kahare (khopo) le tla phola butle, mapetso a tla ba teng mateanong a mabota a kahare le a kantle ha samente e oa;
- (3) Bakeng sa ho thibela likarolo tsa tšepe tse boputsoa ho hlahisa masoba a masoeu, ntle le mehato e nkuoeng ts'ebetsong, botenya ba lebota ha boa lokela ho ba bobebe haholo (lisebelisoa tse ling li bontša hore ha botenya ba lebota bo feta 15mm, Sebelisa likhutlo tse chitja, mme likhutlo tse chitja tsa aluminium alloy le magnesium alloy tšepe hlobo ea tšepe ha ea lokela ho ba tlase ho 3 ~ 4m;
- (4) Ka lebaka la ho se lumellane ha hlobo ea tšepe le mokokotlo, e le ho nolofalletsa ho tlosoa ha letsopa le ho ntšoa ha hlobo, letsoapo la tšepe la tšepe le lokela ho ba le leholo ka mokhoa o nepahetseng ho feta la ho betloa ha lehlabathe, ka kakaretso 30% -50% e kholo. E lokela ho suptjoa: Ntle le mofuta oa motsoako le bophahamo ba lerako, letsoapong la ho betla le amana le boemo ba bokaholimo ba samente. Bokaholimo ba ho betsa bo nang le tšekamelo ea ho ikarola holim'a bokaholimo ba hlobo ea tšepe ha ts'epe e pholile ebile e honyela e ka etsoa ka moepa o monyane. Bokaholimo ba ho betsa, bo atisang ho hatelloa khahlanong le hlobo ea tšepe nakong ea shrinkage, bo lokela ho fuoa letsoapo le leholoanyane.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape: Litaba li hloka tlhokomelo ha ho raloa sebopeho sa ho lahla
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off