Ts'usumetso ea sebopeho sa karolo ea converter dephosphorization slag ho dephosphorization
Ho tloha ha ho qhibilihisoa ha li-phosphorus tsa ultra-low tse kang 9Ni ho na le litlhoko tse tiileng bakeng sa phosphorus ea ho qetela ea sesebelisoa sa tšepe, ho hlokahala hore ka kakaretso e fihlelle phosphorus ea 40 × 10-6 ho converter. Ka hona, Nangang o nka tšepe ea lipeipi e le ntho ea ho etsa lipatlisiso mme a e sebelisa Mokhoeng oa ho qhibilihisa slag + habeli, phosphorus e tšepe e qhibilihisitsoeng e tlosoa haholo nakong ea dephosphorization (one pour).
Phello ea dephosphorization qetellong ea smelting e khethoa ka kotloloho ke phello ea dephosphorization qalong ea smelting. Phetoho ea sebopeho le karolo ea slag nakong eohle ea ts'ebetso ea ho qhibilihisa mofetoleli e bonts'a boemo ba ho qhibiliha le phello ea slag.
Litsebi tse tsoang Univesithing ea Saense le Theknoloji Beijing li sebelisitse thermodynamic software Factsage6.4, SEM, EDS, XRD, e kopantsoe le mekhoa ea liteko tsa infrared le Raman ho sekaseka le ho ithuta sebopeho sa mokhahlelo oa slag ea mantlha le terminal slag. Liphetho li bonts'itse hore viscosity ea slag ea pele le slag ea hoqetela e fokotsehile ka keketseho ea mocheso. Ka mocheso o tšoanang, viscosity ea slag ea pele e ne e le holimo, empa ntlha ea ho qhibiliha e ne e le tlase ho feta ea slag ea ho qetela.
Ho na le mekhahlelo e mengata ea metsi e entsoeng ka mocheso o tlase, e leng se thusang tsoelo-pele ea karabelo ea dephosphorization. Sebaka sa slag Si, Ca, P se ntlafalitsoeng, karolo ea mantlha ea liminerale e thehiloe ke 2CaO • SiO2-3CaO • Karolo ea tharollo e tiileng ea P2O5, e leng molemo haholo ho dephosphorization; ha sebaka sa ntlafatso sa Fe, Mn, Mg le O se ntse se thehoa Mekhahlelo e meholo ke oxide ea tšepe le karolo ea RO, mme bokhoni ba dephosphorization ea slag bo tlase. Liphetho tsa tlhahlobo ea infrared le Raman li bonts'a hore slag ea pele le mofuta oa ho qetela oa slag li-unit tsa SiO4 tetrahedral, slag ea pele e entsoe haholo ka litlamo tsa Si-O-Si, 'me slag ea ho qetela e entsoe ka litlamo tsa POP. Sebopeho sa yuniti ea marang-rang ea silicate e na le molemo o moholo bakeng sa dephosphorization.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape: Ts'usumetso ea sebopeho sa karolo ea converter dephosphorization slag ho dephosphorization
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off