Kakaretso ea lintlha tse fetohang le mekhoa ea taolo ea mofuta oa sebōpi o phatlohang
Mofuta o tloaelehileng oa ts'ebetso ea sebōpi o tšoauoa ka boreleli bo kahare ba lebota le letlalo le tsitsitseng la slag. Leha ho le joalo, tlhahiso ea sebōpi sa 'nete, ka lebaka la tšusumetso ea liphetoho tsamaisong ea ho qhekella, ho tjhaja sistimi, sistimi ea phepelo ea moea, sistimi e futhumatsang le lisebelisoa tse kantle tsa lihlahisoa, mofuta oa sebōpi o sebetsang seboping o tla etsa liphetoho tse joalo ka ho khomarela kapa ho ts'oara slag, e tla ama sebetso sa ho phatloha. Sena se tla baka makhapetla a tebileng a slag, a tla baka tšenyo ea sebaka se seholo sethaleng se pholileng.
Lintlha tsa mantlha tsa khomaretse leboteng ke:
1. Thepa e tala e na le phofshoana e phahameng, phallo ea khase ha e hlahe, 'me phaephe e bohale ea etsahala;
2. Sisteme ea slagging ha e tsitsitse, ts'ebetso ea slag e fetoha haholo, mme slag-iron fluidity e futsanehile, e leng bonolo ho etsa hore lebota la sebōpi le khomarele;
3. Taolo e futsanehileng ea mocheso oa sebōpi, ho fetoha ho hoholo ha maemo, le ho fetoha hoa khafetsa ha sebaka se qhibilihisang sebōpi habonolo.
4. Ho qhibiliha ha nako e telele ea tšepe e phahameng ea silicon le e nang le sebabole se phahameng ho phahameng, 'me slag fluidity e futsanehile;
5. Ho dutla ha lebota le pholileng kapa liphetoho khatellong ea metsi a pholileng le thempereichara ea metsi li baka matla a pholileng a feteletseng;
6. Sisteme ea masela ha e na kahlolo e molemo, e fella ka moea o kenang moeling oa lehae kapa liphaephe tsa bohale.
Mabaka a mantlha a etsang hore letlalo la slag la lebota la sebōpi le oele sebakeng se seholo ke: sistimi ea phepelo ea moea le sistimi ea ho tjhaja ha e na kahlolo e molemo, 'me moea o kenang moeling oa moea o hlaha; phetoho ea sistimi e futhumatsang e baka hore matla a pholileng a be tlase, 'me letlalo le tsitsitseng la slag le ke ke la theoa.
Ha maemo a sebopi a fetoha, ho tlameha ho nkuoe mehato ka nako. Mekhoa e akaretsang ea taolo e sebelisitsoeng ke:
1. Litšobotsi tsa kabo li supa kabo ea phallo ea khase, eo ka eona e khethollang kabo ea sebaka sa mocheso seboping le sebopeho le boemo ba sebaka sa reflow. Haholo-holo boits'oaro bo hlakileng ba tefiso leboteng la sebōpi bo tla etsa hore letlalo la slag le thatafale kapa le oe. Phetoho ea sistimi ea kabo le taolo e sebetsang ea kabo ea phallo ea khase ke mekhoa ea bohlokoa ea ho khutlisetsa mofuta oa sebōpi se tloaelehileng.
Ha lebota la sebōpi le tšoarelletse, ho lokela ho nkuoa mehato e meholo ho beha bohale, 'me moea o kenang moeling o lokela ho ntlafatsoa hantle. Ha letlalo la slag le oela leboteng la sebopi, mehato ea khatello ea bohale e lokela ho nkuoa ho laola phallo ea khase.
Laola mocheso oa sebōpi le motheo oa slag, tšoara khomaretse leboteng, ka nepo laola mocheso oa sebōpi boemong ba moeli o phahameng, ka tieo hanela ts'ebetso e tlase ea mocheso oa sebopi, theola boleng ba slag, 'me sebabole sa tšepe ea kolobe ke karolo ea bobeli. tšepe ho netefatsa botle Mofuthu oa tšepe ea slag.
3. Laola matla a pholileng. Ha letlalo la slag le se bonolo ho theha ha letlalo la slag le oa, khatello ea metsi e lokela ho eketsoa ho eketsa matla a pholileng a karolo eo. Ha tlamo e etsahala, khatello ea metsi e lokela ho fokotsoa ka nepo ho fokotsa matla a pholileng a karolo eo.
4. Ha u sebetsana le ho khomarela karolo e ka tlase, hlatsoa sebōpi hantle
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape:Kakaretso ea lintlha tse fetohang le mekhoa ea taolo ea mofuta oa sebōpi o phatlohang
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off