Liphoso tse 17 tse tloaelehileng ho lahleloa ka tšepe e bonolo
Tlhatlhobo ea Lisosa tsa Mefokolo ho Lisebelisoa tse sa Tšepeheng tsa Tšepe le Tharollo
Tlhahisong ea litšepe tse bonolo tsa tšepe, liphoso tse tloaelehileng tsa ho lahla li kenyelletsa shrinkage cavity, shrinkage porosity, porosity, pores, mapetso, lehlabathe le thellang, bokaholimo ba ho betsa, ho fokotseha, ho haella, sebopeho se fosahetseng, ho tšela ho sa lekanang, ho dutla ha hlobo, molomo o moputsoa, ho phunya, Anti molomo o mosoeu, bohale bo bosoeu bo botenya haholo, ho kheloha, mapheo a teteaneng haholo a oxide, ho robeha hoa mantlha, ho chesa hofeta, ho its'oara, bohale bo hlabang, ho koalla ho sa lekaneng, jj. Hangata, sesosa sa liphoso tsena ha se feela ts'ebetso empa ka linako tse ling ho na le mathata a mangata a ts'ebetso ea tlhahiso joalo ka ho etsa mochini oa mantlha, ho qhibiliha ha smel, boleng ba ho kopanya lehlabathe, ho hloekisa lehlabathe, jj. .
Tlhahisong ea li-castle tse bonolo tsa tšepe, liphoso tse ling tsa li-castings le tlhahlobo ea sesosa le mekhoa ea thibelo ke tse latelang:
1.Shrinkage le shrinkage
Likarolo le mekhoa ea ho sibolla:
Ka hare ho lahla, masoba a manyane a qhalakaneng leboteng le teteaneng le manonyello a chesang a bitsoa shrinkage porosity; masoba a tseparetsoeng a bitsoa likoti tsa shrinkage. Bokaholimo ba lesoba bo bobebe
Tlhahlobo ea Sesosa:
- 1. Ha coke e tlase e theoha, likarolo tsa khabone tsa tšepe e qhibilihisitsoeng li theoha haholo, e leng ho eketsang ho fokotseha
- 2. Sebaka se sa nepahalang sa bophahamo ba metsi, karolo e arolang ea molaleng o nyane haholo, sebaka se pakeng tsa riser le karolo ea phepelo se telele haholo, mme ho lahla ho fepuoa ka mokhoa o sa lekanang.
- 3. Haeba mocheso o tšollang o phahame haholo, tloaelo ea shrinkage porosity le shrinkage cavity e tla eketseha.
- 4. Mongobo oa lehlabathe le holimo haholo, ho kenella hoa moea ho fokotsehile, ho thibelang tšepe e qhibilihisitsoeng ho tlatsa riser, ho fella ka phepelo e sa lekaneng
Mokhoa oa thibelo:
- 1. Ts'ebetso e tsitsitseng ea lik'hemik'hale, taolo ωc lipakeng tsa 2.3% le 2.7%
- 2. Ka kakaretso, tsoho e beoa karolong ea ho qetela e tiisitsoeng ea ho betsa. Karolo e potolohileng ea molala o nyolohang e lokela ho ba e loketseng, 'me bolelele ba molala o nyolohang ka kakaretso ke 5 ~ 8mm
- 3. Khetha mocheso o tšeloang o loketseng
- 4. Laola ka thata mongobo oa lehlabathe le bōpang
Pine ea 2.Dendritic
Likarolo le mekhoa ea ho sibolla:
Lera le ka ntle la ho betsa ke dendritic ebile le hlephile. Ho tloha ka holim'a samente, ho na le likristale tse tšesaane haholo tse kang nale tse supang setsing, e le hore likristale li be le naha e phatsimang. E hlahisoa ka kakaretso haufi le molala o nyolohang, manonyeletso a chesang, li-cores tsa lehlabathe le likhutlo tse bohale tsa castings
Tlhahlobo ea Sesosa:
- 1. Ka kakaretso, sesosa sa dendritic porosity se ts'oana le sa shrinkage porosity, e bakoang haholo ke phepo e sa lekaneng. E amana le botenya ba ho lahla, lik'hemik'hale tsa tšepe e qhibilihisitsoeng, mocheso o tšollang, palo ea aluminium e kenyellelitsoeng le tlhophiso ea riser e tšollang
- 2. Ntle le moo, hobane li-castle tsa tšepe tse bonolo li na le tšepe e tšoeu ea hypoeutectic, sebaka se lipakeng tsa mekhahlelo ea mekhahlelo ea metsi le se tiileng se seholo, se bonolo ho theha li-dendrites. Palo e kholo ea haedrojene e kenella ka tšepe e qhibilihisitsoeng maemong a phahameng. Ha tšepe e entsoeng ka ho qhibilihisoa e tiea, haedrojene e lula bokaholimo ba bokaholimo. Sebopeho sa dendritic porosity
Mokhoa oa thibelo:
- 1. Ho laola ka thata-thata, ka kakaretso e ka bang 0.05%
- 2. Laola ka thata mongobo oa lehlabathe ho ntlafatsa moea o kenang
- 3. Bakeng sa li-castings tse nang le marako a teteaneng, mocheso o tšollang o lokela ho theoloa
- 4. Lihlahisoa tse phahameng tsa silicon le inoculation ho khutsufatsa nako ea ho tiisa
- 5. Hlophisa ka mokhoa o utloahalang sistimi ea ho tšela le riser ho etsa hore phepo e be hantle
3.Stoma le pinhole
Likarolo le mekhoa ea ho sibolla:
Ho lahla ho na le masoba a teteaneng kapa a qhalaneng holim 'a letlalo kapa ka tlasa letlalo,' me bokaholimo ba masoba bo boreleli
Tlhahlobo ea Sesosa:
- 1. Mongobo o mongata haholo lehlabatheng le bōpang, molora o phahameng haholo, le boholo ba phatsa bo botle haholo, bo fokotsang moea o kenang ka lehlabatheng
- 2. Mocheso o tšollelang o tlase haholo, ho tiea ho potlakile, 'me li-bubble ha li bonolo ho baleha
- 3. Haeba likahare tsa mashala a sitsoeng li le holimo haholo, khase e tla ba kholo
- 4. Ho petetsana ha lehlabathe ho phahame haholo kapa moea o kenang kahare ho lehlabathe o tlase
- 5. Ho na le khase e ngata ka tšepe e qhibilihisitsoeng
- 6. Ts'epe e batang ha e hloekile, kapa sebaka ha sea nepahala
Mokhoa oa thibelo:
- 1. Laola mongobo oa lehlabathe le ho ntlafatsa moea o kenang moeeng oa lehlabathe
- 2. Eketsa ka nepo tekanyo ea ho tšela ju
- 3. Laola palo e nepahetseng ea phofo ea mashala
- 4. Fokotsa ka nepo binder ea lehlabathe le bopehileng, le ho tlosa molora lehlabatheng la khale
- 5. Ho kopana ha hlobo ea lehlabathe ho lokela ho ba ho loketseng, 'me moea o kenang moeeng oa lehlabathe o lokela ho matlafatsoa
- 6. Omisa leifo, litlelase tsa pele le lere
- 7. Tšepe e batang e hloka ho hloekisoa le ho hlongoa hantle
4.Pack
Likarolo le mekhoa ea ho sibolla:
Ho na le mapetso a phunyeletsang kapa a sa keneng ka ntle kapa kahare ea samente. Mapatso a chesang a na le bokaholimo bo lefifi kapa bo botšo bo nang le oxidized; mapatso a batang a batla a hloekile ha a na mapetso
Tlhahlobo ea Sesosa:
- 1. Karolo ea khabone e tlase haholo mme shrinkage e kholo haholo
- 2. Ho fepa ho sa lekaneng leboteng le teteaneng la ho lahla kapa ho beha maemo a sa utloahaleng a tšepe e batang
- 3. bōpa lehlabathe kapa lehlabathe konokono na regressivity thusang mafutsana
- 4. Sebabole sa tšepe e entsoeng ka ho qhibilihisoa se phahame haholo, e leng ho eketsang brittleness e chesang
- 5. Heke e kahare e kholo ebile e tsitsitse, 'me palo e nyane, e baka ho chesa ha lehae
- 6. Sebopeho sa ho lahla ha se na kahlolo e molemo 'me botenya ba lerako bo fetoha ka tšohanyetso
- 7. Li-castings li senoloa kapele haholo 'me li pholile ka potlako
- Li-castings li pepesetsoa tšusumetso e matla haholo ha li hloekisoa ke lehlabathe le oang
Mokhoa oa thibelo:
- 1. Taolo ea ωc ha ea lokela ho ba tlase ho 2.3%. Mme ka nepo eketsa mocheso oa tšepe e qhibilihisitsoeng ka seboping le ho fokotsa mocheso o tšollang
- 2. Boemo bo utloahalang ba ho tšela risepe le tšepe e batang
- 3. Hlobo ea lehlabathe ha ea lokela ho ba thata haholo, ea eketsa litekanyo tse lekaneng tsa mapolanka ho ntlafatsa tumellano
- 4. Leka ho boloka lintho tsa sebabole tsa tšepe e entsoeng ka ho qhibilihisoa li le tlase kamoo ho ka khonehang, kapa u laole karolelano e nepahetseng ea manganese le sebabole
- 5. Ntlafatsa sebopeho sa ho lahla, litlhoko tsa phetoho ea botenya ba lebota li fetoha butle-butle
- 6. Eketsa nako ea ho pakolla
- 7. Ha o hloekisa ho betsa, qoba tšusumetso
Leihlo la 5.Scum
Likarolo le mekhoa ea ho sibolla:
Ho na le slag ka masobeng ka ntle kapa kahare ho lahla
Tlhahlobo ea Sesosa:
- 1. slag ka ladle ha e hloekisoe
- 2. slag e ngata haholo ka tšepe e qhibilihisitsoeng
- 3. Phallo e khaoloa nakong ea ho tšela
- Boemo ba sistimi ea gating ha bo utloahale mme phello ea slag ha e ntle
- 5. Sebaka se fosahetseng sa ho tšela
Mokhoa oa thibelo:
- 1. Tlosa masalla ka har'a ladle la letlooa
- 2. Ka nepo eketsa mocheso oa tšepe e qhibilihisitsoeng, palo e nyane ea lehlabathe le ommeng e ka eketsoa ho ladle ea tšepe e qhibilihisitsoeng ho thusa ho tlosoa ha slag e bokelletsoeng.
- 3. Ha u tšela, hlokomela hore u se ke ua emisa ho phalla 'me u boloke senoelo se tletse
- 4. Mokotla oa pokello oa slag o ka beoa ho semathi ho thibela slag
- 5. Likarolo tsa bohlokoa tsa ho betsa li lokela ho beoa ka tlase kapa lehlakoreng
Li-succulents 6
Likarolo le mekhoa ea ho sibolla:
Li-burr tse sa tloaelehang, li-drape kapa li-protrusions tse hlahang
Tlhahlobo ea Sesosa:
- 1. Lehlabathe le ka holimo ha le na matla a lekaneng hore le hlahise mapetso, le baka hore tšepe e qhibilihisitsoeng e phunyeletse
- 2. Pente e mpe
- 3. Ho se lekane ha hlobo ea hlobo kapa tšebeliso e sa lekaneng ea lehlabathe
Mokhoa oa thibelo:
- 1. Sebelisa lehlabathe le letle, 'me ka nepo eketsa nako ea ho kopanya binder le lehlabathe ho eketsa lehlabathe le kaholimo
- 2. Ntlafatsa seaparo
- 3. Ho hlokahala hore lehlabathe le bōpang le be le compactness e ts'oanang le lehlabathe le lekaneng hore le ka jeoa
7. Linaoa tsa tšepe
Likarolo le mekhoa ea ho sibolla:
Ho na le lifaha tse nyane tsa tšepe ka hare ho stomata
- 1. Lehlabathe le etsang metsi le metsi, 'me semathi se ka hare se phahame haholo ho tloha karolong e tlase-tlase ea samente, se etsang hore tšepe e qhibilihisitsoeng e fafatse ebe e etsa linaoa tsa tšepe. Ka mor'a hore tšepe e qhibilihisitsoeng e tlale, linaoa tsa tšepe li ke ke tsa qhibiliha, tsa e etsa hore e koalehe ha e lahleloa ka khase
- 2. Ho kenella hoa moea oa lehlabathe ha ho hotle, 'me khase e hlahisoang e kholo. Ha khase e ngata e hlahisoa ka tšepe e qhibilihisitsoeng, litšepe tse qhibilihisitsoeng, le linaoa tsa tšepe li hlahisoa habonolo holim 'a betse haufi le mokokotlo oa lehlabathe.
Mokhoa oa thibelo:
- 1. Fokotsa mongobo oa lehlabathe le fetisang kapa ho amohela sistimi e tlase ea ho tšela ente hore e kenelle hantle kahare ho fokotsa ho fafatsa tšepe e qhibilihisitsoeng
- 2. Fokotsa ka nepo li-addenda tse nang le khase e kholo ka har'a lehlabathe la mantlha, le ho matlafatsa moea o kenang mohareng oa lehlabathe
8.Ka ho lekaneng ho pholisa le ho tšela
Likarolo le mekhoa ea ho sibolla:
Ho na le likheo kapa khaello ea karolo ea nama ho li-castings tse sa kopaneng ka botlalo, tse nang le mathoko a chitja ho li potoloha
Tlhahlobo ea Sesosa:
- 1. Mocheso o tšollang oa tšepe e qhibilihisitsoeng o tlase haholo
- 2. Lik'hemik'hale tsa tšepe e entsoeng ka ho qhibilihisoa ha lia lokela
- 3. Hlobo ea lehlabathe e metsi haholo
- 4. Sethala sa sistimi ea liheke ha se utloahale, mme karolo ea heke e nyane haholo
- 5. Karolo e 'ngoe ea lebota la tšepe e tšesaane haholo
- 6. Sebaka se fosahetseng sa seporo se batang
- 7. Skew ha u beha mantlha
Mokhoa oa thibelo:
- 1. Eketsa hantle mocheso o tšollang
- Laola lik'hemik'hale tse nepahetseng tsa tšepe e qhibilihisitsoeng
- 3. Fokotsa mongobo lehlabatheng
- 4. Eketsa boholo ba liheke ho potlakisa lebelo la tšollo; bakeng sa castings e telele, tšepe e entsoeng ka ho qhibilihisoa e ka hlahisoa lipheletsong ka bobeli
- 5. Ntlafatsa sebopeho sa ho betsa
- 6. Ka mokhoa o utloahalang hloma tšepe e batang
- 7. Motsoako oa lehlabathe o behiloe ka nepo
9.Cast molomo o moputsoa
Likarolo le mekhoa ea ho sibolla:
Karolo ea ho lahla as-cast e koetsoe kapa e putsoa
Tlhahlobo ea Sesosa:
- 1. Nakong ea ho qhibiliha ha metsoako, metsoako ha e fihlelle litlhokahalo, 'me k'habone le silicone li phahameng haholo
- 2. Ho koala lesela ka nako e sa lekanang nakong ea ho qhibiliha, kapa ho tsoakana ho sa lekaneng ha tšepe e qhibilihisitsoeng
- 3. Botenya ba lebota la samente bo fapane haholo, 'me lebota le teteaneng le tla baka masoba kapa bohlooho.
- 4. Ho pakolla thoto morao haholo
Mokhoa oa thibelo:
- 1. Ho khethiloe mofuta o nepahetseng oa lik'hemik'hale, metsoako ea eona ea utloahala, 'me k'habone le silicone li ka laoloa nakong ea ts'ebetso.
- 2. Kenya se ka pele ho etsa tšepe e qhibilihisitsoeng
- 3. Bakeng sa li-castings tse nang le marako a teteaneng, palo ea bismuth e lokela ho eketsoa ka nepo kapa mocheso o tšollang oa tšepe e qhibilihisitsoeng o lokela ho theoloa
- 4. Phutholla lintho hantle esale pele
10.Castings, e thata ebile e brittle thepa ha e maemong
Likarolo le mekhoa ea ho sibolla:
Thepa ea mochini ha e fihlelle litlhoko tsa sehlopha, haholo bothata bo sa lekaneng le thatafalo e phahameng haholo; cementite e feteletseng kapa lifaha mohahong oa metallographic
'Mele o bobebe; tšepe e nang le lipelo tse ntšo hangata e tšoeu kapa e majabajaba ha e robeha
Tlhahlobo ea Sesosa:
- 1. Motsoako o sa nepahalang oa lik'hemik'hale oa castings, silicon e tlase kapa sebabole se phahameng kapa manganese e phahameng
- 2. Motsoako oa chromium kapa oksijene, naetrojene le haedrojene ea tšepe e qhibilihisitsoeng e feta moeli
- 3. The graphitization annealing ga tlhaloso e fosahetse kapa e laoloa hampe; mokhahlelo oa pele kapa oa bobeli graphitization ha e so phethe
- 4. Taolo e sa nepahalang ha o sebelisa ts'ebetso e tlase ea mocheso oa graphitization
- 5. Decarburization annealing mocheso o tlase haholo kapa taolo e sa nepahalang ea sepakapaka sa decarburization
Mokhoa oa thibelo:
- 1. Laola ka nepo lik'hemik'hale le khase ea tšepe e qhibilihisitsoeng
- Laola ka nepo ts'ebetso ea ho koala graphitization kapa ts'ebetso ea ho fokotsa matla
11. Ho lahla deformation
Likarolo le mekhoa ea ho sibolla:
Kamora ho anetsa, sebopeho le boholo ba samente li fetohile haholo
Tlhahlobo ea Sesosa:
- 1. Ho paka tse sa nepahalang tsa castings
- Mokhahlelo oa pele oa mocheso o kenyang mocheso oa graphitization o holimo haholo 'me nako e telele haholo
- 3. Mocheso oa lehae ka sebōping sa annealing o phahame haholo
Mokhoa oa thibelo:
- 1. Ela hloko mokhoa oa ho paka, eketsa likarolo kapa ho paka
- 2. Fokotsa ka nepo ho senyeha ha sethala sa pele se kenyang graphitization
- 3. Ntlafatsa sebopeho le ts'ebetso ea sebopi sa annealing ho etsa hore mocheso oa sebopi o ts'oane ka hohle kamoo ho ka khonehang
- 4. Fetohela ts'ebetsong ea ho eketsa graphitization ea mocheso o tlase
12.Castings e matla haholo
Likarolo le mekhoa ea ho sibolla:
Sekala se teteaneng sa oxide se thehoa holima samente
Tlhahlobo ea Sesosa:
- 1. Khase ea sebōpi e na le khase e matla
- 2. Lebokose le koalang ha le tiisitsoe hantle
- 3. Mocheso o kenang o holimo haholo 'me nako e telele haholo
Mokhoa oa thibelo:
- 1. Lebokose la annealing le tiisitsoe hantle
- 2. Ha silicone e phahame, theola mocheso o koalang ka nepo
- 3. Laola ka mokhoa o utloahalang karolelano ea manganese-sebabole
- 4. Ho sebelisa mochini o katisang mocheso o tlase oa graphitization
13. Ho hlaseloa ke mantsoe
Likarolo le mekhoa ea ho sibolla:
Bokaholimo ba ho betsa bo bobebe, methapo e qhibilihile, kristale ea fracture e mahoashe, graphite e mahoashe le sebopeho se futsanehile. Ho lahla ho ba bobebe mme thatafalo ea eketseha. Lera la ferrite le nang le oksijene le hlaha ka holim'a samente, eo ka linako tse ling e qhibilihang sebakeng sa heno.
Tlhahlobo ea Sesosa:
- Mokhahlelo oa pele oa mocheso o kenyang mocheso oa graphitization o holimo haholo 'me nako e telele haholo
- 2. Phapang ea mocheso oa sebōpi sa annealing e kholo, 'me mocheso oa sebōpi sebakeng sa lehae o phahame haholo, o fetang melaoana ea ts'ebetso haholo.
Mokhoa oa thibelo:
- 1. Laola sethala sa pele se kenyang mocheso oa graphitization
- 2. Ntlafatsa sebopeho le ts'ebetso ea sebōpi se kenyang letsoho ho etsa seaparo sa mocheso oa sebopi
- 3. Fetohela ts'ebetsong ea ho eketsa graphitization ea mocheso o tlase
Boemo ba brittleness ba 14.
Likarolo le mekhoa ea ho sibolla:
Ho lahla ho na le fracture e tšoeu, 'me ho ba thata ha eona le bophahamo ba eona ho fokotsehile
Tlhahlobo ea Sesosa:
- 1. Kamora mohato oa bobeli oa ho kenya graphitization kapa ho kenya mocheso o tlase, mocheso o theoha butle haholo ho 550 ~ 400 ℃, nako ea bolulo e telele haholo, 'me carbide kapa phosphide e kenella moeling oa lijo-thollo oa ferrite
- 2. Lisebelisoa tsa tšepe li na le phosphorus e phahameng haholo, haholo ha likarolo tsa silicon li phahame, bohale ba ho halefa bo ka etsahala
- 3. Ho chesa ka mokhoa o chesang mochesong oa mocheso (400 ~ 550 ℃) moo ho hlonama ho bang teng
Mokhoa oa thibelo:
- 1. Kamora ho koalisoa, e tla pholisoa kapele ho 600 ~ 650 ℃
- 2. Laola hantle litaba tsa phosphorus, silicon le naetrojene ka tšepe e qhibilihisitsoeng
- 3. Ts'ebetso ea galvanizing e lokela ho qoba moea o bobebe o mocheso. Ha galactic bohale brittleness le hlaha, ho lahla ka replated ho felisa brittleness
- 4. Li-castings tse kileng tsa halefa kapele li ka futhumatsoa ho fihlela li le kaholimo ho 650 ℃ (650 ~ 700 ℃) nako e khuts'oane, ebe li pholile kapele ka seboping, ho thatafala ho ka khutlisoa
15 brittleness ea mocheso o tlase
Likarolo le mekhoa ea ho sibolla:
Mocheso oa phetoho ea maemo a tlase oa metsi o phahama
Tlhahlobo ea Sesosa:
Likahare tsa silicon le phosphorus ha li etsoa li phahame haholo
Mokhoa oa thibelo:
Laola likahare tsa silicon le phosphorus ka castings. Bakeng sa likarolo tse bonolo tsa tšepe tse sebetsang maemong a batang haholo 'me li jara meroalo, ωsi ha ea lokela ho feta 1.7%,' me ωp ha ea lokela ho feta 0.05%
Kabo ea sebopeho sa graphite e futsanehileng
Likarolo le mekhoa ea ho sibolla:
Sebopeho le kabo ea graphite ha li ntle, tse etsang hore thepa ea mochini e hlolehe ho fihlela litlhoko tsa limaraka tse tloaelehileng
Tlhahlobo ea Sesosa:
- 1. Khetho e sa nepahalang ea lik'hemik'hale tsa tšepe e qhibilihisitsoeng
- 2. Kalafo e sa nepahalang ea ente le ts'ebetso ea graphitization
Mokhoa oa thibelo:
- 1. Laola lik'hemik'hale kahare ho sebaka se boletsoeng ho thibela ponahalo ea graphite ea "as-cast"
- 2. Palo ea ente e kenngoang e lokela ho lekana. Ha karoloana e kholo ea boron e feta 0.02%, graphite e bōpehileng joaloka mohala e tla hlaha.
- 3. Mocheso o kenyang letsoho ha oa lokela ho ba holimo haholo, haholoholo mohato oa pele oa graphitization annealing mocheso o lokela ho laoloa ka thata. Haeba e phahame haholo, sebopeho sa graphite se tla senyeha mme palo ea likaroloana e tla fokotseha.
- 4. Sebelisa mokhoa o loketseng oa mocheso o tlase pele o etsoa
Pherekano ea 17.Dendritic
Likarolo le mekhoa ea ho sibolla:
Kamora ho lahla ho kentsoe, ho na le mapetso a manyane a bonahalang kapa a sa bonahaleng ka mahlo, hape ho na le sebopeho se hlephileng sa dendritic se nang le 'mala o hlakileng oa oxidation, o supang holimo ho ea bohareng.
Tlhahlobo ea Sesosa:
Ha ho lahla ho tiisitsoe, ka lebaka la phepelo e sa lekanang ea ho tiisa le maemo a joalo ka sebopeho le kristale, ho thehoa mapetso a manyane a futhumatsang le li-dendrite tse hlephileng. Nakong ea ts'ebetso ea ho koala, khase ea sebōpi e ile ea hlasela mapetsong le likheo tsa dendrite, ea baka ts'oaetso e matla le katoloso e tsoelang pele ea likarolo tse hlephileng.
Mokhoa oa thibelo:
Ntlafatsa kalafo ea ente, hloekisa lijo-thollo, felisa sebopeho sa dendritic le ho ntlafatsa maemo a phepo. Thibela lipoleiti tse kang molomo o mosoeu oa poleiti le ho petsoha ha mocheso.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape:Liphoso tse 17 tse tloaelehileng ho lahleloa ka tšepe e bonolo
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off