The Papiso Of 7 Mefuta shoa Steel
Hona le mefuta e mengata ea tšepe e shoang, 'me mefuta e fapaneng ea lisebelisoa e sebelisoa ka litsela tse fapaneng. Tsebo e ikhethang e hlahisoa ka tlase bakeng sa hau:
Baetsi ba bangata ba polasetiki ba hlobo ba rata botle bo botle ba bokaholimo; ha sebabole se eketsoa ho ntlafatsa ts'ebetso ea ho itšeha ka tšepe, boleng ba bokaholimo bo tla fokotseha ka lebaka leo, 'me tšepe e nang le sebabole se phahameng e tla senyeha haholo.
CRl2
Ts'ebetso ea crl2: kh'habone e phahameng, tšepe e phahameng ea chromium ledeburite, e nang le thatafalo e ntle le ho hanela ho roala hantle. Hobane k'habone ea tšepe e ka fihla ho 2.30%, tšepe e ba thata ebile e brittle, ka hona, ho thatafala ha Chongnan ho fokola, ho thata ho mamella meroalo e meholo, ho bonolo ho robeha, mme ho bonolo ho theha carbides e sa lekanang ea eutectic. .
Ts'ebeliso: E ne e sebelisetsoa ho etsa litebele tse batang le litebele tse nang le litlamorao tse tlase ebile li hloka khatello e phahameng ea ho roala, mahare a batang a ho itšeha bakeng sa ho seha tšepe e thata le e tšesaane, matsoho a ho cheka, mechini e lekanyang, ho taka lintho tse shoang, ho tapa shoela, ho sesa poleiti ea terata, ho taka setopo le nsete phikolosetsa shoela'ng, joalo-joalo
Mefuta ea tlhahiso: Lisebelisoa tse chesang tse chesang, thepa e batang e batang, lisebelisoa tsa ho betla, lipoleiti tsa tšepe tse chesang tse chesang le likhoele tsa tšepe tse huloang ke serame.
CRL2MO1V1
Ts'ebetso: khabone e phahameng, tšepe e phahameng ea chromium ledeburite, ho cheka ha se ntho ea bohlokoa ha ho se na tlhoko e ikhethang. Hobane litaba tsa molybdenum le vanadium li phahame ho feta crl2mov, sebopeho le boholo ba lijo-thollo tsa tšepe li ntlafalitsoe hape, thatafalo, matla le ho tiea ha tšepe li ntlafalitsoe, mme ts'ebetso e phethahetseng ea tšepe e betere.
Ts'ebeliso: E ne e sebelisetsoa ho etsa hlobo e kholo le e rarahaneng ea mosebetsi o batang e hlokang ho itšireletsa haholo, joalo ka lisekere tsa ho itšeha tse batang, ho kuta lintho tse shoang, terata ea kotokaka ea shoa, khoele e sarolohang, khoele e sesa, hemming e shoa, le litebele tse batang lia shoa le litebele tse hlokang holimo apara ho hanyetsa, joalo-joalo.
Mefuta ea tlhahiso: Lisebelisoa tse chesang tse chesang, thepa ea ho betla, thepa e huloang ke serame, lipoleiti tsa tšepe tse chesang tse chesang le likhoele tsa tšepe tse huloang ke serame.
CRL2MOV
Ts'ebetso: Kh'habone e phahameng ea "high-chromium ledeburite", e nang le hardenability e ntle, e ka thatafatsoa ka botlalo ka boholo ba likarolo tse ka tlase ho 400mm, e na le khanyetso e phahameng, 'me e na le liphetoho tse nyane tsa molumo nakong ea ho tima. Karolo ea eona ea khabone e tlase haholo ho feta tšepe ea crl2, mme molybdenum le vanadium lia eketsoa. Ka hona, ho sebetsa ho chesang, ho ba le tšusumetso e thata le ho tsamaisoa ha tšepe ea carbide ho ntlafalitsoe haholo.
Ts'ebeliso: E sebelisetsoa ho etsa hlobo ea mosebetsi o batang ka likarolo tse kholo tsa sefapano, libopeho tse rarahaneng, litlhokahalo tse phahameng tsa ho roala, le mejaro e meholo e matla, joalo ka lisekere tsa ho itšeha tse batang, ho kuta li-die, ho hema, ho shoa, litekanyo, ho taka terata ho shoa, likhoele tsa likhoele, le likhoele Rolling shoa, otla ka litebele shoa ka libopeho rarahaneng, kotokaka tebileng shoa bakeng sa lipoleiti tšepe, 'me otla ka litebele batang shoa le litebele tse hlokang phahameng qhoaele hanyetsa.
Mefuta ea tlhahiso: Lisebelisoa tse chesang tse chesang, thepa ea ho betla, thepa e huloang ke serame, lipoleiti tsa tšepe tse chesang tse chesang le likhoele tsa tšepe tse huloang ke serame.
CR5MOLV
Tshebetso: Lisebelisoa tsa alloy li mahareng. Hobane e na le molybdenum le vanadium, tšepe e na le hardenability e ntle, kabo ea junifomo ea carbide, khatello e itseng ea ts'usumetso le ho hanela ho roala hantle.
Ts'ebeliso: e sebelisetsoang ho etsa li-shiling, li-sleeve tsa ho cheka, litebele tse batang lia shoa, litebele, ho kuta li shoa, khoele e sarolohang, lipolanka tse potang, li-gauges, jj.
Mefuta ea tlhahiso: Lisebelisoa tse chesang tse chesang, thepa ea ho betla, thepa e huloang ke serame, lipoleiti tsa tšepe tse chesang tse chesang le likhoele tsa tšepe tse huloang ke serame.
9MN2V
Ts'ebetso: Ha e bapisoa le tšepe ea sesebelisoa sa khabone, likarolo tse phethahetseng tsa mochini li na le thatafalo e phahameng le ho roala, ho thatafala hantle, le ho senyeha ho fokolang nakong ea ho tima. Hobane tšepe e na le vanadium e itseng, lithollo tsa kristale lia hloekisoa mme kutloisiso ea ho chesa haholo ea fokotseha. Ho se lekane ha carbide ho molemo ho feta tšepe ea crwmn.
Ts'ebeliso: E sebelisetsoa ho etsa lisebelisoa tse fapaneng tsa ho lekanya ka nepo, litempele, 'me ka kakaretso ho hlokahala lisiti tse nyane, mochini o hatisang o batang oa shoa, mongolo o shoa, lintho tse shoang, sekere, pompo, shoa le li-reamers, jj.
Mefuta ea tlhahiso: Lisebelisoa tse chesang tse chesang, thepa ea ho betla, thepa e huloang ke serame, lipoleiti tsa tšepe tse chesang tse chesang le likhoele tsa tšepe tse huloang ke serame.
Li-module tse nyane le tse mahareng li ka fanoa ho latela litlhoko tsa moreki.
LEKHOTLA
Tshebetso: E na le hardenability e phahameng. Hobane 1.20% ~ 1.60% (karoloana ea boima) ea tungsten e eketsoa ho theha carbides, e na le thatafalo e itseng mme e apara ho hanyetsa kamora ho tima le mocheso o tlase oa mocheso. Tungsten e thusa ho boloka lijo-thollo tse ntle, hore tšepe e be le thata e thata, tšepe e nahanela sebopeho sa matlooa a khabone, 'me mofuta ona oa letlooa la sechaba la khabone o etsa hore sesebelisoa e be karolo ea kotsi ea ho qhalana.
Morero: Sebelisa mefuta e fapaneng ea mesebetsi e batang ea tšepe. E sebelisetsoa ho etsa lisebelisoa tsa ho lekanya, tse kang die, gauge gauge, sampole kholomo le sleeve ea sampole, 'me sebetsa ka mokhoa o nepahetseng se shoa ka libopeho tse rarahaneng.
Mefuta ea tlhahiso: lisebelisoa tse chesang tse chesang, thepa ea ho betla, thepa e huloang ke serame, lithapo tsa tšepe tse huloang ke serame, lithapo tsa tšepe tse khanyang ka tšepe, maqephe a tšepe a chesang, le maqephe a tšepe a batang.
9CRWMN
Tshebetso: Low-alloy e batang-e sebetsa tšepe, e nang le ho thatafala ho itseng le ho apara ho hanyetsa, phetoho e nyane ea quenching, kabo ea junifomo ea carbide le likaroloana tse ntle.
Ts'ebeliso: E sebelisetsoa ho etsa lisepa tse batang tse batang ka likarolo tse nyane tsa sefapano le libopeho tse rarahaneng, hammoho le lisebelisoa tsa ho lekanya tse kang litekanyo le lipampiri.
Mefuta ea tlhahiso: Lisebelisoa tse chesang tse chesang, thepa ea ho betla, thepa e huloang ke serame, lithapo tsa tšepe tse huloang ke serame le lipoleiti tsa tšepe tse batang.
Ka kopo boloka mohloli le aterese ea sengoloa sena hore se hatisoe hape:The Papiso Of 7 Mefuta shoa Steel
Minghe Khamphani ea Die Casting li inehetse ho etsa le ho fana ka boleng bo phahameng le likarolo tse phahameng tsa ho lahla likarolo Thining-Wall Die Casting,Hot Chamber Die lahla,Cold Chamber shoa lahla), Tšebeletso e chitja (Die Casting Service,Cnc Machining,Ho Etsa Mofuta, Bokaholimo Phekolo) .Na tloaelo efe kapa efe ea Aluminium die die cast, magnesium kapa Zamak / zinc die casting le litlhoko tse ling tsa castings lia amoheleha ho ikopanya le rona
Tlas'a taolo ea ISO9001 le TS 16949, lits'ebetso tsohle li etsoa ka mechini e makholo ea li-die casting, mechini e 5-axis le lits'ebeletso tse ling, ho tloha ho li-blasters ho isa mechini ea ho hlatsoa ea Ultra Sonic. sehlopha sa baenjiniere ba nang le boiphihlelo, lisebelisoa le bahlahlobi ho etsa moralo oa moreki o phethahala.
Moetsi oa konteraka oa li-cast cast. Bokhoni bo kenyelletsa likarolo tse batang tsa aluminium die die likarolo tsa 0.15 lbs. ho isa ho li-6 lbs., Ho theha phetoho e potlakileng, le machining. Litšebeletso tse kenyellelitsoeng boleng li kenyelletsa ho bentsa, ho thothomela, ho qhekella, ho phatloha ha lithunya, ho penta, ho roala, ho roala, kopano le lisebelisoa. Lisebelisoa tse sebelisitsoeng le tsona li kenyelletsa lits'epe tse kopantsoeng tse kang 360, 380, 383 le 413.
Zinc e shoa ho lahla thuso ea moralo / lits'ebeletso tsa boenjineri tse tšoanang. Moetsi oa moetlo oa li-castings tsa zinc tse nepahetseng. Li-castings tse nyane, li-castings tse phahameng tsa khatello, li-cast cast tsa hlobo, li-castings tse tloaelehileng tsa hlobo, li-unit tsa die le li-cast cast tse ikemetseng le li-cast cast tse tiisitsoeng li ka etsoa. Li-castings li ka etsoa ka bolelele le bophara ho fihlela 24 ho. Ho +/- 0.0005 ho. Mamello.
ISO 9001: Moetsi ea netefalitsoeng oa 2015 oa magnesium ea die die, Bokhoni bo kenyelletsa khatello e phahameng ea khatello ea magnesium die cast to 200 ton room & 3000 kamoreng e batang, moralo oa lithulusi, polishing, molding, machining, powder & liquid paint, QA e felletseng e nang le bokhoni ba CMM , kopano, ho paka le ho tsamaisa.
ITAF16949 e netefalitsoe. Ts'ebeletso e 'ngoe ea ho lahla e kenyeletsa ho lahla lichelete,ho lahla lehlabathe,Matla a khoheli, Lahlehileng bubble lahla,Ho ts'oaroa ha Centrifugal,lephaka lahla,Sa Feleng hlobo lahlaBokhoni bo kenyelletsa EDI, thuso ea boenjiniere, ho etsa mohlala o tiileng le ho sebetsoa ka bobeli.
Lahla Liindasteri Liphuputso tsa likarolo tsa likarolo tsa: Likoloi, libaesekele, lifofane, liletsa tsa 'mino, sesepa sa metsi, lisebelisoa tsa Optical, li-sensor, mehlala, lisebelisoa tsa elektroniki, masaka, lioache, mechini, lienjine, thepa ea ka tlung, mabenyane, mabenyane, telecom, mabone, lisebelisoa tsa bongaka, lisebelisoa tsa litšoantšo, Liroboto, Litšoantšo tse betliloeng, Lisebelisoa tsa molumo, Lisebelisoa tsa lipapali, Lithulusi, Lipapali le tse ling.
Re ka u thusa ho etsa eng ka mor'a moo?
∇ Eya ho Homepage Bakeng sa Shoa lahla China
→Likarolo tsa ho lahla-Fumana seo re se entseng.
→ Malebela a Ralated ka Litšebeletso tsa Die Casting
By Moetsi oa Minghe Die Casting | Categories: Lingoloa tse thusang |lintho tse bonahalang Tags: Aluminium lahla, Ho lahla zinki, Ho lahla Magnesium, Lahleloa thaethaniamo, Ho lahla tšepe, Brass lahla,Ho lahleloa ka Bronze,Ho lahla Video,Histori ea Khamphani,Aluminium Die Casting | Litlhaloso Off