Liphoso tse 5 tse Tloaelehileng Mokhoeng oa Die Carburizing
Palo ea li-austenite tse bolokiloeng ke le leng la mabaka a ho ba thata ho tlase ha setempe. Palo ea li-austenite tse bolokiloeng ka lera la carburized hangata e bakoa ke mocheso o phahameng oa carburizing le mohopolo o phahameng oa khabone, o lebisang bothateng bo tlase ba setepe se shoang. E nngwe ...